Physical Properties | Metric | English | Comments |
---|
Density | 1.37 g/cc | 0.0495 lb/in³ |
Filler Content | 30 % | 30 % |
Linear Mold Shrinkage, Flow | 0.0010 - 0.0030 cm/cm | 0.0010 - 0.0030 in/in |
Linear Mold Shrinkage, Transverse | 0.0070 - 0.0090 cm/cm | 0.0070 - 0.0090 in/in |
|
Mechanical Properties | Metric | English | Comments |
---|
Tensile Strength at Break | 100 MPa | 14500 psi |
| 145 MPa | 21000 psi |
Elongation at Break | 3.0 % | 3.0 % |
| 4.0 % | 4.0 % |
Tensile Modulus | 7.60 GPa | 1100 ksi |
| 10.0 GPa | 1450 ksi |
Charpy Impact Unnotched | 7.90 J/cm² @Temperature 23.0 °C | 37.6 ft-lb/in² @Temperature 73.4 °F |
|
Electrical Properties | Metric | English | Comments |
---|
Dielectric Strength | 15.0 kV/mm @Thickness 1.00 mm | 381 kV/in @Thickness 0.0394 in |
| 15.0 kV/mm @Thickness 1.00 mm | 381 kV/in @Thickness 0.0394 in |
Comparative Tracking Index | >= 600 V | >= 600 V |
Hot Wire Ignition, HWI | >= 120 sec @Thickness 0.800 mm | >= 120 sec @Thickness 0.0315 in |
| >= 120 sec @Thickness 0.400 mm | >= 120 sec @Thickness 0.0157 in |
| >= 120 sec @Thickness 1.60 mm | >= 120 sec @Thickness 0.0630 in |
| >= 120 sec @Thickness 3.20 mm | >= 120 sec @Thickness 0.126 in |
| >= 120 sec @Thickness 0.400 mm | >= 120 sec @Thickness 0.0157 in |
| >= 120 sec @Thickness 1.60 mm | >= 120 sec @Thickness 0.0630 in |
| >= 120 sec @Thickness 3.20 mm | >= 120 sec @Thickness 0.126 in |
| >= 120 sec @Thickness 0.800 mm | >= 120 sec @Thickness 0.0315 in |
High Amp Arc Ignition, HAI | >= 120 arcs @Thickness 0.400 mm | >= 120 arcs @Thickness 0.0157 in |
| >= 120 arcs @Thickness 0.800 mm | >= 120 arcs @Thickness 0.0315 in |
| >= 120 arcs @Thickness 1.60 mm | >= 120 arcs @Thickness 0.0630 in |
| >= 120 arcs @Thickness 3.20 mm | >= 120 arcs @Thickness 0.126 in |
| >= 120 arcs @Thickness 0.400 mm | >= 120 arcs @Thickness 0.0157 in |
| >= 120 arcs @Thickness 0.800 mm | >= 120 arcs @Thickness 0.0315 in |
| >= 120 arcs @Thickness 1.60 mm | >= 120 arcs @Thickness 0.0630 in |
| >= 120 arcs @Thickness 3.20 mm | >= 120 arcs @Thickness 0.126 in |
|
Thermal Properties | Metric | English | Comments |
---|
Melting Point | 260 °C | 500 °F |
Deflection Temperature at 0.46 MPa (66 psi) | 261 °C | 502 °F |
Deflection Temperature at 1.8 MPa (264 psi) | 245 °C | 473 °F |
UL RTI, Electrical | 65.0 °C @Thickness 0.400 mm | 149 °F @Thickness 0.0157 in |
| 65.0 °C @Thickness 0.800 mm | 149 °F @Thickness 0.0315 in |
| 65.0 °C @Thickness 1.60 mm | 149 °F @Thickness 0.0630 in |
| 65.0 °C @Thickness 3.20 mm | 149 °F @Thickness 0.126 in |
| 65.0 °C @Thickness 0.400 mm | 149 °F @Thickness 0.0157 in |
| 65.0 °C @Thickness 0.800 mm | 149 °F @Thickness 0.0315 in |
| 65.0 °C @Thickness 1.60 mm | 149 °F @Thickness 0.0630 in |
| 65.0 °C @Thickness 3.20 mm | 149 °F @Thickness 0.126 in |
UL RTI, Mechanical with Impact | 65.0 °C @Thickness 0.400 mm | 149 °F @Thickness 0.0157 in |
| 65.0 °C @Thickness 0.800 mm | 149 °F @Thickness 0.0315 in |
| 65.0 °C @Thickness 1.60 mm | 149 °F @Thickness 0.0630 in |
| 65.0 °C @Thickness 3.20 mm | 149 °F @Thickness 0.126 in |
| 65.0 °C @Thickness 0.400 mm | 149 °F @Thickness 0.0157 in |
| 65.0 °C @Thickness 0.800 mm | 149 °F @Thickness 0.0315 in |
| 65.0 °C @Thickness 1.60 mm | 149 °F @Thickness 0.0630 in |
| 65.0 °C @Thickness 3.20 mm | 149 °F @Thickness 0.126 in |
UL RTI, Mechanical without Impact | 65.0 °C @Thickness 0.400 mm | 149 °F @Thickness 0.0157 in |
| 65.0 °C @Thickness 0.800 mm | 149 °F @Thickness 0.0315 in |
| 65.0 °C @Thickness 1.60 mm | 149 °F @Thickness 0.0630 in |
| 65.0 °C @Thickness 3.20 mm | 149 °F @Thickness 0.126 in |
| 65.0 °C @Thickness 0.400 mm | 149 °F @Thickness 0.0157 in |
| 65.0 °C @Thickness 0.800 mm | 149 °F @Thickness 0.0315 in |
| 65.0 °C @Thickness 1.60 mm | 149 °F @Thickness 0.0630 in |
| 65.0 °C @Thickness 3.20 mm | 149 °F @Thickness 0.126 in |
Flammability, UL94 | V-0 @Thickness 0.800 mm | V-0 @Thickness 0.0315 in |
| V-0 @Thickness 0.400 mm | V-0 @Thickness 0.0157 in |
| V-0 @Thickness 1.60 mm | V-0 @Thickness 0.0630 in |
| V-0 @Thickness 3.20 mm | V-0 @Thickness 0.126 in |
| V-0 @Thickness 0.400 mm | V-0 @Thickness 0.0157 in |
| V-0 @Thickness 1.60 mm | V-0 @Thickness 0.0630 in |
| V-0 @Thickness 3.20 mm | V-0 @Thickness 0.126 in |
| V-0 @Thickness 0.800 mm | V-0 @Thickness 0.0315 in |
Glow Wire Ignition Temperature | 750 °C @Thickness 0.400 mm | 1380 °F @Thickness 0.0157 in |
| 750 °C @Thickness 0.800 mm | 1380 °F @Thickness 0.0315 in |
| 750 °C @Thickness 1.60 mm | 1380 °F @Thickness 0.0630 in |
| 750 °C @Thickness 3.20 mm | 1380 °F @Thickness 0.126 in |
| 750 °C @Thickness 0.400 mm | 1380 °F @Thickness 0.0157 in |
| 750 °C @Thickness 0.800 mm | 1380 °F @Thickness 0.0315 in |
| 750 °C @Thickness 1.60 mm | 1380 °F @Thickness 0.0630 in |
| 750 °C @Thickness 3.20 mm | 1380 °F @Thickness 0.126 in |
Glow Wire Flammability Index | 960 °C @Thickness 0.400 mm | 1760 °F @Thickness 0.0157 in |
| 960 °C @Thickness 0.800 mm | 1760 °F @Thickness 0.0315 in |
| 960 °C @Thickness 1.60 mm | 1760 °F @Thickness 0.0630 in |
| 960 °C @Thickness 3.20 mm | 1760 °F @Thickness 0.126 in |
| 960 °C @Thickness 0.400 mm | 1760 °F @Thickness 0.0157 in |
| 960 °C @Thickness 0.800 mm | 1760 °F @Thickness 0.0315 in |
| 960 °C @Thickness 1.60 mm | 1760 °F @Thickness 0.0630 in |
| 960 °C @Thickness 3.20 mm | 1760 °F @Thickness 0.126 in |