Recently Viewed Materials
AGC Fluon® LM-730AP LM-ETFE Fluororesin
(discontinued **)
Categories:
Polymer
;
Thermoplastic
;
Fluoropolymer
;
ETFE/ECTFE
;
Modified ETFE, Unreinforced
Material Notes:
Fluon®LM-ETFE combines the excellent properties in heat resistance and other mechanical properties owned by ETFE resin and the low melting point.
Information provided by Asahi Glass Company, Inc.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Specific Gravity
1.78
g/cc
1.78
g/cc
ASTM D792
Melt Flow
20
-
30
g/10 min
20
-
30
g/10 min
ASTM D359
Mechanical Properties
Metric
English
Comments
Tensile Strength at Break
40.0
MPa
5800
psi
ASTM D638
Elongation at Break
400 %
400 %
ASTM D638
Flexural Modulus
0.647
GPa
93.8
ksi
ASTM D790
Izod Impact, Notched
NB
NB
ASTM D256
Electrical Properties
Metric
English
Comments
Dielectric Constant
2.4
@Frequency 1000 Hz
2.4
@Frequency 1000 Hz
ASTM D150
2.4
@Frequency 1e+6 Hz
2.4
@Frequency 1e+6 Hz
ASTM D150
Dissipation Factor
0.00070
@Frequency 1000 Hz
0.00070
@Frequency 1000 Hz
ASTM D150
0.0082
@Frequency 1e+6 Hz
0.0082
@Frequency 1e+6 Hz
ASTM D150
Thermal Properties
Metric
English
Comments
Melting Point
225
°C
437
°F
Flammability, UL94
V-0
V-0
Oxygen Index
40 %
40 %
ASTM D2863
Descriptive Properties
10% Weight Loss °C
410
Anti cracking at 200°C
excellent
Heat Ageing (retention of elongation)
120%
Heat Ageing (retention of tensile strength)
88%
**
Materials flagged as discontinued (
) are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.
Users of our Advanced Search (registration required) may exclude discontinued materials from search results.
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
AGC Fluon® LM-720AP LM-ETFE Fluororesin
AGC Fluon® LH-8000 ETFE
Vycom FLAMETEC™ HALAR® 901 Opaque Ethylene Chlorotrifluoroethylene (ECTFE)
AGC Fluon® LM-740AP LM-ETFE Fluororesin
AGC Fluon® LM-740A ETFE
PAGC15 / 22974
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.