MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

13Cr-4.5Mo-0.75Ti-6Al-2.3(Nb+Ta)-Zr-B NICKEL BASED SUPERALLOY CASTINGS FOR GAS TURBINE BLADES
Categories: Metal; Ferrous Metal; Tool Steel; Air-Hardening Steel

Material Notes:

Creep and rupture data provided by NIMS

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Rupture Strength  33.0 - 40.0 MPa
@Temperature 975 °C,
Time 3.60e+8 sec
4790 - 5800 psi
@Temperature 1790 °F,
Time 100000 hour
 31.0 - 50.0 MPa
@Temperature 950 °C,
Time 3.60e+8 sec
4500 - 7250 psi
@Temperature 1740 °F,
Time 100000 hour
 39.0 - 62.0 MPa
@Temperature 925 °C,
Time 3.60e+8 sec
5660 - 8990 psi
@Temperature 1700 °F,
Time 100000 hour
 50.0 - 77.0 MPa
@Temperature 900 °C,
Time 3.60e+8 sec
7250 - 11200 psi
@Temperature 1650 °F,
Time 100000 hour
 63.0 - 94.0 MPa
@Temperature 875 °C,
Time 3.60e+8 sec
9140 - 13600 psi
@Temperature 1610 °F,
Time 100000 hour
 79.0 - 116 MPa
@Temperature 850 °C,
Time 3.60e+8 sec
11500 - 16800 psi
@Temperature 1560 °F,
Time 100000 hour
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 5.0 - 7.0 %5.0 - 7.0 %
Boron, B <= 0.025 %<= 0.025 %
Chromium, Cr 12 - 14 %12 - 14 %
Iron, Fe 69.6 - 77 %69.6 - 77 %As Balance
Molybdenum, Mo 3.5 - 5.5 %3.5 - 5.5 %
Nb + Ta 2.0 - 2.6 %2.0 - 2.6 %
Titanium, Ti 0.50 - 1.25 %0.50 - 1.25 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
MetalTek IN® 713 UNS N07713 Centri-Vac Nickel Cobalt Based Alloy
20Cr-20Ni-20Co-4W-4Mo-4(Nb+Ta) IRON BASED SUPERALLOY BARS FOR GAS TURBINE BLADES
19Cr-18Co-4Mo-3Ti-3Al-B NICKEL BASED SUPERALLOY CASTINGS AND FORGINGS FOR GAS TURBINE BLADES
Alloy 713C Cast Nickel Superalloy (UNS N07713)
IN-738 Cast Nickel Superalloy

NIMS032 / 77549

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.