MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

DAK Americas Laser+® C (E60A) PET
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET); Polyethylene Terephthalate (PET), Unreinforced

Material Notes: Product Description: Laser+® C (E60A) is a unique copolymer particularly suited for use in the custom PET container applications where clarity and neutral colored are desired. It is a medium intrinsic viscosity (IV) product that gives the end user a strong clear bottle and offers excellent processing and consistency.

Typical Properties: Bi-orientation of Laser+® C (E60A) by injection/stretch blow molding provides optimal barrier and mechanical properties, including excellent vacuum performance. It performs well in both single- and two-stage processes used in the manufacturing of PET containers. Laser+® C (E60A) offers excellent clarity and color, while maintaining good reheat characteristics for stretch blow molding. In addition, because it is a copolymer resin, it offers reduced crystallization rates and a wide processing window.

Certification: Laser+® C (E60A) is ideally suited for food packaging applications and is considered in compliance with the Food and Drug Administration (FDA) Food Contact Notification (FCN) 000635, covering PET polymers

Information provided by DAK Americas

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.870 g/cc0.0314 lb/in³DAK-QAR-SOP-0018
Particle Size 3000 µm3000 µmFlat Cylinder Shape; DAK-QAR-SOP-0017
Particle Mesh Size 24 Mesh24 MeshFines: <0.1%, as packaged; DAK-QAR-SOP-0014
Viscosity Test 79 - 83 cm³/g0.79 - 0.83 dl/gIntrinsic; DAK-QAR-SOP-0012
Crystallinity >= 50 %>= 50 %DAK-QAR-SOP-0016
 
Thermal PropertiesMetricEnglishComments
Melting Point 246 °C475 °Fnominal; DAK-QAR-SOP-0016
 
Processing PropertiesMetricEnglishComments
Moisture Content <= 0.25 %<= 0.25 %DAK-QAR-SOP-0013; as packaged
 
Descriptive Properties
Chip Size48-58 chips/gnominal, DAK-QAR-SOP-0015
Color-5.0- -1.0 CIEb*, DAK-QAR-SOP-0011
 85-89 CIEL*, DAK-QAR-SOP-0011
Compounds<2 ppmAcetaldehyde, DAK-QAR-SOP-0010

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
DAK Americas Laser+® C (C60A) PET
Wellman PermaClear™ 61803 (0.81 IV) PET
DAK Americas Laser+® C 9921 (F65A) PET

PDAKA016 / 147991

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.