MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Angst+Pfister APSOplast® PUR D44 90 Sh. A Polyester urethane (AU)
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Chemically, PUR D44 is based on polyester polyol + diphenylmethane-4.4-diisocyanate (DESMODUR® 44). PUR D44 is a high-quality polyurethane with good abrasion resistance and structural strength. In comparison with PUR D15, this material is somewhat cheaper and more resistant to hydrolysis but less suitable for parts exposed to dynamic stress. PUR D44 should not be used at a long-term temperature of over +80 °C. However, short-term exposure to temperatures of up to +100 °C is possible. This material has a hardness of between approx. 65 Shore A and 60 Shore D.

Information provided by Angst + Pfister

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 9090DIN 53505
Tensile Strength at Break 29.0 MPa4210 psiDIN 53504
Tensile Stress at Strain  2.95 MPa
@Strain 20 %
428 psi
@Strain 20 %
DIN 53504
 13.7 MPa
@Strain 300 %
1990 psi
@Strain 300 %
DIN 53504
Elongation at Break 500 %500 %DIN 53504
Tear Strength 60.0 kN/m342 pliDIN 53515
Abrasion 4444[mm3]; DIN 53516

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PANGP111 / 250609

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.