MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Pitch Pine Wood
Categories: Wood and Natural Products; Wood; Softwood

Material Notes: Also known as longleaf yellow pine or longleaf pitch pine or American pitch pine. Test material of southern USA origin.
Usual surface texture: Medium
Dimensional changes when dried lumber is subjected to variations in humidity during service: Medium
Resistance to fungal decay (Heartwood in ground contact): Moderately Durable (10 to 15 years)
Resistance to penetration by preservatives: Resistant
Common Applications: Interior and exterior joinery, heavy construction

Key Words: Pinus palustris, Pinus Elliottii, Pinus Resinosa; Red Pine, Lumber, Timber
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.554 - 0.740 g/cc0.0200 - 0.0267 lb/in³at nominal specific gravity
 0.716 g/cc0.0259 lb/in³at oven-dry state
 0.747 g/cc0.0270 lb/in³Nominal; at 10.0% m.c.
 0.673 - 0.900 g/cc0.0243 - 0.0325 lb/in³at 10.0% m.c.
Moisture Absorption at Equilibrium 3.0 - 7.5 %3.0 - 7.5 %Between 40% RH and 90% RH
 
Mechanical PropertiesMetricEnglishComments
Poissons Ratio 0.3080.308µTR, 12% Moisture Content
 0.3150.315µLT, 12% Moisture Content
 0.3470.347µLR, 12% Moisture Content
 0.4080.408µRT, 12% Moisture Content
Machinability 50 %50 %Medium Relative to Other Wood
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.121 W/m-K0.840 BTU-in/hr-ft²-°FOven Dry, US origin
 0.144 W/m-K1.00 BTU-in/hr-ft²-°F12% Moisture Content, US origin
Shrinkage 4.0 %4.0 %Radial, from green to oven dry, US origin
 7.1 %7.1 %Tangential, from green to oven dry, US origin
 10.9 %10.9 %Volumetric, from green to oven dry, US origin
 
Descriptive Properties
ColorYellow-brown to red-brownUsual for heartwood

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
American Pine Wood
European Black Pine (Austrian Pine) Wood
Red Pine Wood
Southern Pine Wood
Northern White Pine Wood

PTSM009 / 71362

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.