MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

ASI® Pipe Sealer TORQUE 177 Anaerobic Methacrylate Adhesive
Categories: Polymer; Adhesive; Thermoset; Methacrylate; Methacrylate Adhesive

Material Notes: TORQUE 177 is a Anaerobic curing adhesive for the a sealing of thread joints. Replaces PTFE tape and yarn, gives instant sealing against moderate pressure, gives flexible cured film. Seals against gas, water, LPG, hydrocarbons, oils and other chemicals. Thixotropic property prevents migration from thread of the sealant before or during curing. Shocks and vibrations resistances are unaffected properties of sealing in the range of temperature from -50 to +150°C.

Information provided by Adhesive Systems, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.05 g/cc0.0379 lb/in³uncured
Viscosity 90000 cP
@Temperature 25.0 °C
90000 cP
@Temperature 77.0 °F
thixotropic. Uncured
 
Mechanical PropertiesMetricEnglishComments
Shear Strength 6.00 - 13.0 MPa870 - 1890 psi
Coefficient of Friction 0.130.13uncured
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 150 °C302 °F
Minimum Service Temperature, Air -55.0 °C-67.0 °F
Flash Point >= 100 °C>= 212 °Funcured
 
Processing PropertiesMetricEnglishComments
Cure Time 5.00 - 10.0 min0.0833 - 0.167 hourhandling. Cured
 180 - 360 min3.00 - 6.00 hourFunctional
Shelf Life 12.0 Month
@Temperature 25.0 °C
12.0 Month
@Temperature 77.0 °F
uncured
 
Descriptive Properties
Chemical ClassAnaerobic Methacrylate
Color / appearancewhite
Fluorescenceunder blue light
Locking Torque10-14 N., prevailing.
 18-22 Nm, breakaway.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PASINC9190 / 233556

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.