MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

HGC-1-C Precious dental alloy
Categories: Metal; Nonferrous Metal; Precious Metal; Gold Alloy

Key Words: medical, surgical
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 18.3 - 18.6 g/cc0.661 - 0.672 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Vickers 60 - 7560 - 75soft
 70 - 9070 - 90hardened
Tensile Strength, Ultimate 220 - 280 MPa31900 - 40600 psisoft
Tensile Strength, Yield 230 - 300 MPa33400 - 43500 psihardened
 90.0 - 130 MPa
@Strain 0.2 %
13100 - 18900 psi
@Strain 0.2 %
soft
 105 - 140 MPa
@Strain 0.2 %
15200 - 20300 psi
@Strain 0.2 %
hardened
Elongation at Break 27 - 38 %27 - 38 %hardened
 29 - 38 %29 - 38 %soft
 
Thermal PropertiesMetricEnglishComments
CTE, linear 14.1 - 14.8 µm/m-°C
@Temperature 25.0 - 600 °C
7.83 - 8.22 µin/in-°F
@Temperature 77.0 - 1110 °F
Melting Point 1090 - 1370 °C1990 - 2500 °F
Solidus 1090 °C1990 °F
Liquidus 1370 °C2500 °F
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 0.00 - 5.0 %0.00 - 5.0 %
Gold, Au 50 - 73 %50 - 73 %
Indium, In <= 2.0 %<= 2.0 %
Iridium, Ir <= 0.10 %<= 0.10 %
Palladium, Pd <= 1.0 %<= 1.0 %
Platinum, Pt <= 1.9 %<= 1.9 %
Rhenium, Re <= 0.10 %<= 0.10 %
Silver, Ag 10 - 28 %10 - 28 %
Zinc, Zn 12 - 14 %12 - 14 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
HGC-4 Precious dental alloy
HGC-1 Precious dental alloy
HGC-3 Precious dental alloy
AgPd-4 Precious dental alloy
AgPd-1 Precious dental alloy

MMEDIC34 / 12410

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.