MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Asahi Kasei Stylac™ 190F ABS Polymer, High Flow
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Molded

Material Notes:

Information provided by Asahi Kasei Corp.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.05 g/cc0.0379 lb/in³ISO 1183
Linear Mold Shrinkage 0.0040 - 0.0060 cm/cm0.0040 - 0.0060 in/inASTM D955
Melt Flow 47 g/10 min
@Load 9.18 kg,
Temperature 220 °C
47 g/10 min
@Load 20.2 lb,
Temperature 428 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 100
@Thickness 2.50 mm
100
@Thickness 0.0984 in
Tensile Strength, Yield 46.0 MPa6670 psi50mm/min; ISO 527-1
Flexural Strength 69.0 MPa10000 psi2mm/min; ISO 178
Flexural Modulus 2.25 GPa326 ksi2mm/min; ISO 178
Charpy Impact, Notched 1.70 J/cm²8.09 ft-lb/in²ISO 179
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 60.0 °C140 °FRelative Thermal Index; UL 746A
Hot Ball Pressure Test 85.0 °C185 °FRegistered Number: B-1556; EMAC
Deflection Temperature at 1.8 MPa (264 psi) 74.0 °C165 °FISO 75-1,2
Vicat Softening Point 91.0 °C
@Load 5.10 kg
196 °F
@Load 11.2 lb
ISO 306
Flammability, UL94 HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Hannam Chemical Hanalac 780 ABS, High Flow
I. Stern 728 High Gloss Medium Natural ABS
Elix Polymers Elix™ 118HF ABS Polymer
Ecomass® 720ZD88 Tungsten Filled ABS
Asahi Kasei Stylac™ IB330 ABS Polymer, Extrusion, Blow Molding

PASAHI8261 / 221285

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.