MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Overview of materials for Medium Carbon Steel
Categories: Metal; Ferrous Metal; Carbon Steel; Medium Carbon Steel

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Medium Carbon Steel". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.75 - 7.89 g/cc0.280 - 0.285 lb/in³Average value: 7.85 g/cc Grade Count:917
Particle Size 6.70 - 12.0 µm6.70 - 12.0 µmAverage value: 9.27 µm Grade Count:12
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 126 - 578126 - 578Average value: 247 Grade Count:831
Hardness, Knoop 145 - 616145 - 616Average value: 276 Grade Count:838
Hardness, Rockwell B 71.0 - 11271.0 - 112Average value: 94.8 Grade Count:779
Hardness, Rockwell C 9.00 - 71.09.00 - 71.0Average value: 25.9 Grade Count:703
Hardness, Vickers 131 - 614131 - 614Average value: 265 Grade Count:838
Tensile Strength, Ultimate 450 - 2730 MPa65300 - 396000 psiAverage value: 986 MPa Grade Count:838
Tensile Strength, Yield 230 - 1740 MPa33400 - 252000 psiAverage value: 684 MPa Grade Count:831
Elongation at Break 5.00 - 34.2 %5.00 - 34.2 %Average value: 18.9 % Grade Count:822
Reduction of Area 20.0 - 71.4 %20.0 - 71.4 %Average value: 49.7 % Grade Count:529
Modulus of Elasticity 187 - 213 GPa27100 - 30900 ksiAverage value: 203 GPa Grade Count:902
Bulk Modulus 152 - 163 GPa22000 - 23600 ksiAverage value: 160 GPa Grade Count:863
Poissons Ratio 0.280 - 0.3000.280 - 0.300Average value: 0.290 Grade Count:887
Fatigue Strength 138 - 614 MPa20000 - 89100 psiAverage value: 350 MPa Grade Count:16
Fracture Toughness 80.9 - 143 MPa-m½73.7 - 130 ksi-in½Average value: 120 MPa-m½ Grade Count:4
Machinability 40.0 - 80.0 %40.0 - 80.0 %Average value: 60.1 % Grade Count:641
Shear Modulus 72.0 - 82.0 GPa10400 - 11900 ksiAverage value: 79.6 GPa Grade Count:894
Izod Impact 9.00 - 135 J6.64 - 99.6 ft-lbAverage value: 45.7 J Grade Count:256
Charpy Impact 10.8 - 65.0 J8.00 - 47.9 ft-lbAverage value: 31.7 J Grade Count:8
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000166 - 0.0000263 ohm-cm0.0000166 - 0.0000263 ohm-cmAverage value: 0.0000213 ohm-cm Grade Count:798
 
Thermal PropertiesMetricEnglishComments
CTE, linear 10.4 - 15.1 µm/m-°C5.78 - 8.39 µin/in-°FAverage value: 12.9 µm/m-°C Grade Count:595
Specific Heat Capacity 0.470 - 0.519 J/g-°C0.112 - 0.124 BTU/lb-°FAverage value: 0.477 J/g-°C Grade Count:619
Thermal Conductivity 21.9 - 52.0 W/m-K152 - 361 BTU-in/hr-ft²-°FAverage value: 47.7 W/m-K Grade Count:713
Melting Point 1420 - 1460 °C2590 - 2660 °FAverage value: 1440 °C Grade Count:3
Maximum Service Temperature, Air 400 °C752 °FAverage value: 400 °C Grade Count:3
 
Processing PropertiesMetricEnglishComments
Processing Temperature 166 - 838 °C331 - 1540 °FAverage value: 600 °C Grade Count:8
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 0.0200 - 1.15 %0.0200 - 1.15 %Average value: 0.324 % Grade Count:4
Boron, B 0.000500 - 0.00300 %0.000500 - 0.00300 %Average value: 0.00175 % Grade Count:43
Carbon, C 0.100 - 1.29 %0.100 - 1.29 %Average value: 0.418 % Grade Count:955
Chromium, Cr 0.130 - 4.50 %0.130 - 4.50 %Average value: 0.829 % Grade Count:597
Cobalt, Co 4.50 - 8.00 %4.50 - 8.00 %Average value: 6.60 % Grade Count:5
Copper, Cu 0.200 - 0.500 %0.200 - 0.500 %Average value: 0.300 % Grade Count:9
Iron, Fe 78.7 - 100 %78.7 - 100 %Average value: 97.4 % Grade Count:955
Manganese, Mn 0.100 - 3.00 %0.100 - 3.00 %Average value: 0.912 % Grade Count:952
Molybdenum, Mo 0.0300 - 4.25 %0.0300 - 4.25 %Average value: 0.266 % Grade Count:476
Nickel, Ni 0.150 - 10.0 %0.150 - 10.0 %Average value: 1.13 % Grade Count:294
Phosphorus, P 0.00800 - 0.400 %0.00800 - 0.400 %Average value: 0.0363 % Grade Count:921
Silicon, Si 0.0500 - 2.20 %0.0500 - 2.20 %Average value: 0.294 % Grade Count:669
Sulfur, S 0.00200 - 0.500 %0.00200 - 0.500 %Average value: 0.0546 % Grade Count:924
Vanadium, V 0.0300 - 1.00 %0.0300 - 1.00 %Average value: 0.176 % Grade Count:57

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Low Carbon Steel
Overview of materials for High Carbon Steel
Overview of materials for Stainless Steel
Overview of materials for Low Alloy Steel
Overview of materials for AISI 4000 Series Steel

M01011 / 81729

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.