MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

A. Schulman BMC 810 General Purpose Molding Compound
Categories: Polymer; Thermoset; Polyester, TS; Thermoset Polyester Glass and Mineral Filled BMC

Material Notes: BMC 810 is a general purpose, very high strength compound suitable for compression, transfer and stuffer injection molding. It is characterized by excellent flow and controlled reactivity and is well suited for injection molding.

Typical applications include structural components, mechanical applications, and bearing plates.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.75 - 1.85 g/cc1.75 - 1.85 g/cc
Water Absorption 0.15 - 0.25 %0.15 - 0.25 %24 hours, 23°C
Linear Mold Shrinkage 0.0010 - 0.0030 cm/cm0.0010 - 0.0030 in/in
 
Mechanical PropertiesMetricEnglishComments
Hardness, Barcol 45 - 5245 - 52
Tensile Strength, Ultimate 68.9 - 82.7 MPa10000 - 12000 psi
Elongation at Yield 2.0 - 2.5 %2.0 - 2.5 %Tensile
Flexural Strength 165 - 186 MPa24000 - 27000 psi
Flexural Modulus 11.7 - 13.1 GPa1700 - 1900 ksi
Compressive Strength 131 - 152 MPa19000 - 22000 psi
Izod Impact, Notched 7.47 - 9.08 J/cm14.0 - 17.0 ft-lb/in
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 16.7 kV/mm425 kV/inShort Time
Arc Resistance >= 180 sec>= 180 sec
Comparative Tracking Index >= 500 V>= 500 V
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) >= 232 °C>= 450 °F
Flammability, UL94 V-0V-0
 
Processing PropertiesMetricEnglishComments
Mold Temperature 138 - 166 °C280 - 330 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Thermoset Polyester Glass Filled BMC
A. Schulman BMC 304 Automotive Grade Molding Compound
A. Schulman BMC 200 Thermoset Polyester, Electrical Grade
A. Schulman BMC 102 Glass Filled Thermoset Polyester
Overview of materials for Thermoset Polyester Glass and Mineral Filled BMC

PBMC033 / 27216

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.