MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Flame Retardant adhesives

Sumitomo Bakelite SUMILITE® ELC-4970 Glass Epoxy Laminate
Categories: Polymer; Thermoset; Epoxy; Epoxy/Glass SMC

Material Notes: Glass Epoxy Double sided Materials for PCB

Information provided by Sumitomo Bakelite High Performance Plastics (sbhpp)

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Water Absorption 0.090 %0.090 %E-24/50+D-24/23
 
Mechanical PropertiesMetricEnglishComments
Tensile Modulus 12.0 GPa1740 ksiTD
 14.0 GPa2030 ksiMD
Flexural Strength 300 MPa43500 psiTD
 350 MPa50800 psiMD
Flexural Modulus 16.0 GPa2320 ksiTD
 18.0 GPa2610 ksiMD
Peel Strength 1.50 kN/m8.56 pliA; 18umCF
 1.50 kN/m8.56 pliS-20"/260; 18umCF
Film Tensile Strength at Break, MD 160 MPa23200 psi
Film Tensile Strength at Break, TD 100 MPa14500 psi
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant  4.1
@Frequency 1e+9 Hz
4.1
@Frequency 1e+9 Hz
C-96/20/65
 4.2
@Frequency 1e+9 Hz
4.2
@Frequency 1e+9 Hz
C-96/20/65+D-24/23
 4.5
@Frequency 1e+6 Hz
4.5
@Frequency 1e+6 Hz
C-96/20/65
 4.5
@Frequency 1e+6 Hz
4.5
@Frequency 1e+6 Hz
C-96/20/65+D-24/23
Dissipation Factor  0.018
@Frequency 1e+9 Hz
0.018
@Frequency 1e+9 Hz
C-96/20/65
 0.019
@Frequency 1e+9 Hz
0.019
@Frequency 1e+9 Hz
C-96/20/65+D-24/23
 0.020
@Frequency 1e+6 Hz
0.020
@Frequency 1e+6 Hz
C-96/20/65
 0.022
@Frequency 1e+6 Hz
0.022
@Frequency 1e+6 Hz
C-96/20/65+D-24/23
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 84.6 µm/m-°C47.0 µin/in-°F10°C/min; Z (a1)
 540 µm/m-°C300 µin/in-°F10°C/min; Z (a2)
CTE, linear, Transverse to Flow 36.0 µm/m-°C20.0 µin/in-°F10°C/min; X (a1)
 43.2 µm/m-°C24.0 µin/in-°F10°C/min; Y (a1)
Glass Transition Temp, Tg 125 °C257 °F10°C/min
 130 °C266 °F20°C/min
 150 °C302 °F5°C/min
Flammability, UL94 V-0V-0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Sumitomo Bakelite SUMILITE® PLC-2147 AQ Paper Phenolic
Sumitomo Bakelite SUMILITE® PLC-2147 RF Paper Phenolic
Sumitomo Bakelite SUMILITE® ELC-4762 Glass Epoxy
Sumitomo Bakelite SUMILITE® ELC-4768/EI-6768 Glass Epoxy Laminate
Sumitomo Bakelite SUMILITE® ELC-4972R&S Glass Epoxy Laminate

PSUMIT116 / 193921

Flame Retardant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.