MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Chi Mei Polylac® PA-764G ABS Resin
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant

Material Notes: Highly flame retardant, high heat resistance, 0.75mm V-2, 1.0mm V-0, 2.5mm 5VA. Applications: Displays, machine boxes, modems, power panels, power outlets, car batteries, cash register shells, printer casings, remote control, light boxes, fax machines, projectors, large-scale multifunctional peripherals, coffee machine, front and rear TV frames, DVD players, car audio consoles.

POLYLAC® ABS resin is a copolymer primarily composed of styrene (SM), acrylonitrile (AN), and butadiene (BD). ABS has very good mechanical properties, dimensional stability, processing ability, chemical resistance, and a high-quality appearance.

Information provided by Chi Mei Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.22 g/cc0.0441 lb/in³ISO 1183
Linear Mold Shrinkage 0.0030 - 0.0060 cm/cm0.0030 - 0.0060 in/inISO 294-4
Melt Flow 34 g/10 min34 g/10 minMelt Volume Rate (ml/10 min.); ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 27.0 MPa3920 psi50mm/min; ISO 527
Tensile Strength, Yield 34.0 MPa4930 psi50 mm/min; ISO 527
Elongation at Break 10 %10 %50mm/min; ISO 527
Flexural Strength 54.0 MPa7830 psi2mm/min; ISO 178
Flexural Modulus 1.80 GPa261 ksi2 mm/min; ISO 178
Izod Impact, Notched (ISO)  7.00 kJ/m²
@Temperature -30.0 °C
3.33 ft-lb/in²
@Temperature -22.0 °F
ISO 180/1A
 13.0 kJ/m²
@Temperature 23.0 °C
6.19 ft-lb/in²
@Temperature 73.4 °F
ISO 180/1A
Charpy Impact, Notched  0.700 J/cm²
@Temperature -30.0 °C
3.33 ft-lb/in²
@Temperature -22.0 °F
ISO 179
 1.20 J/cm²
@Temperature 23.0 °C
5.71 ft-lb/in²
@Temperature 73.4 °F
ISO 179
 
Thermal PropertiesMetricEnglishComments
CTE, linear 83.0 µm/m-°C46.1 µin/in-°FISO 11359
Deflection Temperature at 1.8 MPa (264 psi) 82.0 °C180 °FUnannealed; ISO 75/A
 92.0 °C198 °FAnnealed; ISO 75/A
Vicat Softening Point  90.0 °C
@Load 5.00 kg
194 °F
@Load 11.0 lb
50°C/hr; ISO 306
 101 °C
@Load 1.00 kg
214 °F
@Load 2.20 lb
50°C/hr; ISO 306
Flammability, UL94  V-2
@Thickness 0.750 mm
V-2
@Thickness 0.0295 in
 V-0
@Thickness 1.00 mm
V-0
@Thickness 0.0394 in
 5VA
@Thickness 2.50 mm
5VA
@Thickness 0.0984 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCHI9929 / 280819

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.