MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

A. Schulman FORMION™ FI 233 15% Mineral Reinforced Ionomer / Nylon Alloy
Categories: Polymer; Thermoplastic; Ionomer; Nylon (Polyamide PA)

Material Notes: Description

Formion® FI 233 is an injection molding grade, 15% mineral reinforced Ionomer / Nylon alloy, which has been formulated for high scratch resistance, heat resistance and high stiffness.
Application

Formion® FI 233 is targeted for non painted, mold-in-color, exterior or interior appearance applications.
Information provided by A. Schulman.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.15 g/cc1.15 g/ccISO 1183/1
Linear Mold Shrinkage 0.0010 - 0.0060 cm/cm
@Thickness 3.20 mm
0.0010 - 0.0060 in/in
@Thickness 0.126 in
aged 48 hrs at 121°C; ISO 294
 0.0050 - 0.0090 cm/cm
@Thickness 3.20 mm,
Time 259000 sec
0.0050 - 0.0090 in/in
@Thickness 0.126 in,
Time 72.0 hour
ISO 294
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 47.0 MPa6820 psiISO 527
Elongation at Break 170 %170 %ISO 527
Flexural Modulus 2.60 GPa377 ksiTangent; ISO 178
Izod Impact, Notched (ISO) 19.1 kJ/m²9.09 ft-lb/in²ISO 180
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 122 °C
@Thickness 3.17 mm
252 °F
@Thickness 0.125 in
ISO 75

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
NYCOA 2263 Copolymer Nylon Alloy
NYCOA 1838 Copolymer Nylon Alloy
Envalior Arnitel® VT3104 TPC-ET, Extrusion Grade
Envalior Arnitel® UM551 55 Shore D Copolyester Elastomer (North America)
Envalior Arnitel® EB463 Polyether Ester Elastomer (European and Asian Grade)

PASHU029 / 24993

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.