MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Chevron Phillips Marlex® K203 LLDPE Sheet Extrusion  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Extrusion Grade

Material Notes: Resin Type: Hexene Copolymer

Characteristics:

  • Outstanding ESCR
  • Broad fusion range
  • Excellent melt strength
  • Good processability
  • Excellent flexibility
  • Improved output and texturing

Applications:

  • Coextruded cap layers for HDPE
  • Blends with HDPE
  • Landfill covers and caps
  • Masterbatch projects
  • Round and flat die projects

Information provided by Chevron Phillips.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.922 g/cc0.0333 lb/in³ASTM D1505
ESCR 100% Igepal® >= 1500 hour>= 1500 hourCondition C; ASTM D1693
ESCR 10% Igepal® >= 1500 hour>= 1500 hourCondition B; ASTM D1693
Melt Flow 15 g/10 min15 g/10 minCondition 190/21.6, HLMI; ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 5555ASTM D2240
Tensile Strength, Yield 12.0 MPa1740 psi2 in/min, Type IV bar; ASTM D638
Elongation at Break 750 %750 %2 in/min, Type IV bar; ASTM D638
Flexural Modulus 0.480 GPa69.6 ksiTangent, 16:1 span:depth,0.5in/min; ASTM D790
Tensile Impact Strength 800 kJ/m²381 ft-lb/in²Type S bar; ASTM D1822
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 51.0 °C124 °FMethod A; ASTM D648
Vicat Softening Point 104 °C219 °FLoading 1, Rate A; ASTM D1525
Brittleness Temperature <= -75.0 °C<= -103 °FType A clamp, type 1 specimen; ASTM D746
 
Descriptive Properties
SP-NCTLMin 1000Single-point notched constant tensile load

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow DNDB-7441 NT 7 Linear Low Density Polyethylene Resin
A. Schulman CP814-01 Linear, Low-Density Polyethylene
Chevron Phillips Marlex® 9398 HDPE Pipe and Corrugated Extrusion Resin
Chevron Phillips Marlex® 9519H High Density Polyethylene, Blow Molding
Chevron Phillips Marlex® C514 HDPE Pipe and Corrugated Extrusion Resin

PCHEVD042 / 20647

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.