MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Daikin PTFE M-532 Polytetrafluoroethylene Molding Powder
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE); Polytetrafluoroethylene (PTFE), Molded

Material Notes: Daikin PTFE M-532 is a polytetrafluoroethylene virgin granular free flow resin. M-532 has excellent powder flow characteristics and may be used successfully for compression molding, automatic molding, isostatic molding and ram extrusion applications.

Information provided by Daikin.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.15 - 2.17 g/cc2.15 - 2.17 g/ccASTM D 4894
Bulk Density 0.840 g/cc0.0303 lb/in³ASTM D 4894
Particle Size 350 - 550 µm350 - 550 µm
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break >= 30.0 MPa>= 4350 psiJIS K6891
Elongation at Break >= 300 %>= 300 %JIS K6891
 
Thermal PropertiesMetricEnglishComments
Shrinkage 2.5 - 3.5 %2.5 - 3.5 %
 
Descriptive Properties
AppearanceWhite Powder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Rogers Arlon 99-108065 PTFE Resin
Dalau Dalcon 020 Virgin PTFE, Carbon (Anti-Static)
AGC Fluon® FC 182 PTFE, Bronze powder/ Molybdenum Disulfide Filled

PDAIJ9882 / 209953

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.