MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Techmer ES Luriblend® HTN 05007
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); High Temperature Nylon

Material Notes: Availability: North America

Forms: Pellets

Additive: Heat Stabilizer and Lubricant

Features: Heat Stabilized, High Heat Resistance and Lubricated

Appearance: Black

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.17 g/cc0.0423 lb/in³ASTM D792
Water Absorption 0.25 %
@Time 86400 sec
0.25 %
@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.016 cm/cm
@Thickness 3.17 mm
0.016 in/in
@Thickness 0.125 in
ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 114114ASTM D785
Tensile Strength, Yield 67.6 MPa9800 psiASTM D638
Elongation at Break 50 %50 %ASTM D638
Flexural Strength 96.5 MPa14000 psiASTM D790
Flexural Modulus 2.28 GPa330 ksiASTM D790
Izod Impact, Notched 0.427 J/cm
@Thickness 3.17 mm
0.800 ft-lb/in
@Thickness 0.125 in
ASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmASTM D257
Surface Resistance 1.00e+14 ohm1.00e+14 ohmASTM D257
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 84.6 µm/m-°C47.0 µin/in-°FASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 224 °C435 °FUnannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 121 °C250 °FUnannealed; ASTM D648
Flammability, UL94 V-2V-2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTPC0772 / 136710

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.