MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Vermiculite, Magnesium Aluminum Iron Silicate
Categories: Ceramic; Oxide; Magnesium Oxide; Silicon Oxide

Material Notes: Vermiculite is the name given to one of several hydrous laminar minerals. When heated, vermiculite expands (exfoliates) due to the pressure of escaping steam. Control of the exfoliation conditions allows the properties of the exfoliated product to be controlled to suit specific applications. Exfoliated vermiculite is a very absorbent material - water or other liquids can be absorbed in the atomic level layers.

Vermiculite is found worldwide. The properties reported below are from the Phalaborwa deposit.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.0560 - 0.160 g/cc0.00202 - 0.00578 lb/in³Exfoliated; Higher grades have a lower bulk density
 0.600 - 1.10 g/cc0.0217 - 0.0397 lb/in³Bulk ore prior to exfoliation
Density 2.50 g/cc0.0903 lb/in³
Loss On Ignition  4.5 - 6.5 %
@Temperature 105 °C
4.5 - 6.5 %
@Temperature 221 °F
 8.0 - 10 %
@Temperature 950 °C
8.0 - 10 %
@Temperature 1740 °F
pH 8.0 - 9.58.0 - 9.5
Specific Surface Area 7.7 - 50 m²/g7.7 - 50 m²/gExfoliated; Higher grades have a higher specific surface area
 
Mechanical PropertiesMetricEnglishComments
Hardness, Mohs 1.0 - 2.01.0 - 2.0
 
Thermal PropertiesMetricEnglishComments
Specific Heat Capacity 1.08 J/g-°C0.258 BTU/lb-°F
Thermal Conductivity 0.0620 - 0.0650 W/m-K0.430 - 0.451 BTU-in/hr-ft²-°FExfoliated
Melting Point 1330 °C2430 °F
 
Component Elements PropertiesMetricEnglishComments
Al2O3 8.0 - 9.5 %8.0 - 9.5 %
CaO 2.0 %2.0 %
Chlorine, Cl <= 0.050 %<= 0.050 %
CO2 1.5 %1.5 %
Cr2O3 0.15 %0.15 %
Fe2O3 5.0 - 6.0 %5.0 - 6.0 %
Fluorine, F 0.60 %0.60 %
H2O, Water 8.0 - 10 %8.0 - 10 %
K2O 4.0 - 6.0 %4.0 - 6.0 %
MgO 24.5 - 27 %24.5 - 27 %
P2O5 0.060 %0.060 %
SiO2 38 - 40 %38 - 40 %
TiO2 0.75 %0.75 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Fused Quartz
Yttria Stabilized Zirconia, YSZ
Zirconium Oxide, Zirconia, ZrO2
Concrete, exfoliated vermiculite aggregate
Nickel silver 65-10, UNS C74500, OSO35, Temper flat products

BVERMIC0 / 324

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.