Metallocene Medium Density High Gloss Blow Molding Resin Characteristics: - Outstanding gloss
- Good flexibility
- Excellent impact strength
- Good ESCR
- USP Class VI compliant
- FDA Compliant
Applications: - Coextruded Glossy Bottles
- Monolayer Squeezable Bottles
- Injection Blow Molded Containers
This former Total Petrochemicals grade is now a part of the Bayport Polymers joint venture. |
Outstanding gloss; Good flexibility |