MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Potassium Sodium Niobate, K0.5Na0.5NbO3
Categories: Ceramic; Oxide; Silicon Oxide

Material Notes:

Key Words: potassium sodium niobium oxide, K0.5Na0.5NbO3
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 4.25 g/cc0.154 lb/in³air fired
 4.46 g/cc0.161 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Modulus of Elasticity 104 GPa15100 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+12 ohm-cm1.00e+12 ohm-cm
Dielectric Constant  290
@Frequency 100000 Hz
290
@Frequency 100000 Hz
air fired
 420
@Frequency 100000 Hz
420
@Frequency 100000 Hz

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Calcium Hydroxyapatite, Ca10(PO4)6(OH)2
Hornblende (Iron-Magnesium Silicate)
Mica (K(Mg,Fe)3(AlSi3O10)(OH)2)
Mica (KAl2(AlSi3O10)(OH)2)
Olivine, Peridot ((Mg, Fe)2SiO4)

BN1A / 252

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.