Omnix® LF-4050 BK 000-9 is a 50% Long Glass Fiber reinforced, easy-flowing, heat stabilized HPPA with a very high flexural modulus. It exhibits stiffness/toughness combination, an excellent retention of properties in a wide temperature range as well as outstanding creep and fatigue resistance. Omnix® LF-4050 BK 000-9 has a pellet length of 9mm and can be processed on most injection-molding machines. Key Attributes: Creep Resistant; Electrically Insulating; Fatigue Resistant; High Impact Resistance; High Temperature Stiffness; Hot Water Moldability; Low CLTE; Low Shrinkage; Low Warpage Applications: Aircraft Applications; Automotive Applications; Consumer Applications; Industrial Applications Injection Notes: Pre-Drying -- Since polyamides are hygroscopic materials as well as sensitive to moisture during processing, this product should always be pre-dried. Recommended drying time is 4 hours at 120°C in dry-air dryer. Regrind -- Regrind of highly filled thermoplastic materials, such as this material, should only be recycled with special care. The regrind content must never exceed 20% and only regrind of optimum quality should be used. In any case, part properties should be checked. Data for dry samples unless noted. Information provided by Solvay Specialty Polymers. |