MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Syensqo (Solvay Specialty Polymers) Omnix® LF-4050 BK 000-9 Polyamide, High Performance (HPPA), 50% Long Glass Fiber  (Unverified Data**)
Categories: Polymer; Thermoplastic; Polyphthalamide (PPA); Polyphthalamide (PPA), 50% Glass Fiber Reinforced

Material Notes: Omnix® LF-4050 BK 000-9 is a 50% Long Glass Fiber reinforced, easy-flowing, heat stabilized HPPA with a very high flexural modulus. It exhibits stiffness/toughness combination, an excellent retention of properties in a wide temperature range as well as outstanding creep and fatigue resistance.

Omnix® LF-4050 BK 000-9 has a pellet length of 9mm and can be processed on most injection-molding machines.

Key Attributes: Creep Resistant; Electrically Insulating; Fatigue Resistant; High Impact Resistance; High Temperature Stiffness; Hot Water Moldability; Low CLTE; Low Shrinkage; Low Warpage

Applications: Aircraft Applications; Automotive Applications; Consumer Applications; Industrial Applications

Injection Notes: Pre-Drying -- Since polyamides are hygroscopic materials as well as sensitive to moisture during processing, this product should always be pre-dried. Recommended drying time is 4 hours at 120°C in dry-air dryer.

Regrind -- Regrind of highly filled thermoplastic materials, such as this material, should only be recycled with special care. The regrind content must never exceed 20% and only regrind of optimum quality should be used. In any case, part properties should be checked.

Data for dry samples unless noted.

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.59 g/ccISO 1183
Moisture Absorption 1.40 %50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0010 cm/cmISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 235 MPa
@Temperature 23.0 °C
Conditioned; ISO 527-2
 270 MPa
@Temperature 23.0 °C
ISO 527-2
Elongation at Break 2.0 %Conditioned; ISO 527-2
 2.1 %ISO 527-2
Tensile Modulus 17500 MPa
@Temperature 23.0 °C
Conditioned; ISO 527-2
 17500 MPa
@Temperature 23.0 °C
ISO 527-2
Flexural Strength 360 MPa
@Temperature 23.0 °C
ISO 178
Flexural Modulus 16000 MPa
@Temperature 23.0 °C
ISO 178
Charpy Impact Unnotched 95.0 kJ/m²
@Temperature 23.0 °C
Conditioned; ISO 179
 95.0 kJ/m²
@Temperature 23.0 °C
ISO 179
Charpy Impact, Notched 35.0 kJ/m²
@Temperature 23.0 °C
Conditioned; ISO 179
 35.0 kJ/m²
@Temperature 23.0 °C
ISO 179
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 35.0 kV/mm
@Thickness 2.00 mm
IEC 60243-1
Comparative Tracking Index 600 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 20.0 µm/m-°CISO 11359-2
Thermal Conductivity 0.320 W/m-KISO 8302
Deflection Temperature at 0.46 MPa (66 psi) 260 °CUnannealed; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 255 °CUnannealed; ISO 75-2/A
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 280 - 300 °C
Middle Barrel Temperature 285 - 300 °C
Front Barrel Temperature 285 - 300 °C
Nozzle Temperature 285 - 300 °C
Melt Temperature <= 320 °C
Mold Temperature 80.0 - 140 °C
Drying Temperature 80.0 °C
@Time 14400 - 43200 sec
Moisture Content <= 0.10 %
 
Descriptive Properties
Availability (as of March 2019)Africa & Middle East; Asia Pacific; Europe; Latin America; North America
ColorBlack
FormsPellets
ProcessingInjection Molding
Suggested Max Regrind Injection (%)20

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSOL8Y5258 / 238639

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.