MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
CRP  Windform
Envalior Novamid® ID 1030 Nylon 6/66, 3D Printing Grade
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6/66

Material Notes: This is a filament grade - not available for sale as granules.

Novamid® material for Fused Filament Fabrication (FFF), produces parts almost indistinguishable from those produced with standard injection molding.

This open source filament material is a pure polyamide 6/ 66, and was developed for demanding specialty applications often subjected to harsh environment and high temperatures (up to 125°C).

Optimized to 3D-print easily, Novamid® ID 1030 filaments bring a combination of properties, including outstanding stiffness and ductility, across a range of applications - from transportation, to sports and electronics. Their optimized crystallization profile improves fusion, enabling parts with excellent interlayer strength and high surface quality.

Unless specified as a comment, data refer to dry testing conditions.

Former DSM Engineering Plastics product line is now with Envalior.

Vendors:
Available Properties
  • Density, ISO 1183
  • Water Absorption, Sim. to ISO 62
  • Moisture Absorption, Sim. to ISO 62
  • Viscosity Number, ISO 307, 1157, 1628
  • Melt Flow, ISO 1133
  • Tensile Strength at Break, ISO 527-1/-2, Dry
  • Tensile Strength at Break, ISO 527-1/-2, Conditioned
  • Tensile Strength, Ultimate, ISO 527-1/-2, 3D printed tensile bars, 45°-45°
  • Tensile Strength, Yield, ISO 527-1/-2, Conditioned
  • Tensile Strength, Yield, ISO 527-1/-2, Dry
  • Elongation at Break, ISO 527-1/-2, Dry
  • Elongation at Break, ISO 527-1/-2, Conditioned
  • Elongation at Break, ISO 527-1/-2, 3D printed tensile bars, 45°-45°
  • Elongation at Yield, ISO 527-1/-2, Dry
  • Elongation at Yield, ISO 527-1/-2, Conditioned
  • Tensile Modulus, ISO 527-1/-2, Conditioned
  • Tensile Modulus, ISO 527-1/-2, 3D printed tensile bars, 45°-45°
  • Tensile Modulus, ISO 527-1/-2, Dry
  • Flexural Strength, ISO 178, Conditioned
  • Flexural Strength, ISO 178, Dry
  • Flexural Modulus, ISO 178, Conditioned
  • Flexural Modulus, ISO 178, Dry
  • Charpy Impact Unnotched, ISO 179/1eU
  • Charpy Impact Unnotched, ISO 179/1eU
  • Charpy Impact, Notched, ISO 179/1eA, Conditioned
  • Charpy Impact, Notched, ISO 179/1eA, Dry
  • Charpy Impact, Notched, ISO 179/1eA, Dry
  • Charpy Impact, Notched, ISO 179/1eA, Conditioned
  • Melting Point, ISO 11357-1/-3, 10°C/min
  • Deflection Temperature at 0.46 MPa (66 psi), ISO 75-1/-2
  • Deflection Temperature at 1.8 MPa (264 psi), ISO 75-1/-2
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Envalior, former LANXESS

Category Notes
Plastic
PA, Polyamide

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.