This is a filament grade - not available for sale as granules. Novamid® material for Fused Filament Fabrication (FFF), produces parts almost indistinguishable from those produced with standard injection molding. This open source filament material is a pure polyamide 6/ 66, and was developed for demanding specialty applications often subjected to harsh environment and high temperatures (up to 125°C). Optimized to 3D-print easily, Novamid® ID 1030 filaments bring a combination of properties, including outstanding stiffness and ductility, across a range of applications - from transportation, to sports and electronics. Their optimized crystallization profile improves fusion, enabling parts with excellent interlayer strength and high surface quality. Unless specified as a comment, data refer to dry testing conditions. Former DSM Engineering Plastics product line is now with Envalior. |
Proto3000 provides design tools, 3D printers, additive manufacturing processes, metrology technologies, high-performance materials, and part-finishing automation. Our ISO 9001:2015 additive manufacturing production facility offers 3D printing services, rapid prototyping services, and end-part production with HP MultiJet Fusion (MJF), FDM, SLA, SLS, Polyjet, DLP, metal binder jetting, BMD, and DMLS.Click here to view all available suppliers for this material.Please click here if you are a supplier and would like information on how to add your listing to this material. |