LNP STAT-KON DX05474 compound is based on Polycarbonate (PC) resin containing 10% carbon fiber. Added features of this grade include: Electrically Conductive, Easy Molding, Flame Retardant, Mold Release. Features: Light-weight Structural,Super Strong (Carbon Fiber Filled),Flame Retardant,Good Mold Release,Exceptional Processing,Electrically Conductive,Easy Molding Information provided by SABIC |