MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

SABIC LNP™ STAT-KON™ Compound DX05474 Polycarbonate (PC)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: LNP STAT-KON DX05474 compound is based on Polycarbonate (PC) resin containing 10% carbon fiber. Added features of this grade include: Electrically Conductive, Easy Molding, Flame Retardant, Mold Release.

Features: Light-weight Structural,Super Strong (Carbon Fiber Filled),Flame Retardant,Good Mold Release,Exceptional Processing,Electrically Conductive,Easy Molding

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.29 g/cc0.0466 lb/in³ASTM D792
 1.29 g/cc0.0466 lb/in³ISO 1183
Moisture Absorption 0.0200 %0.0200 %Injection Molding
Linear Mold Shrinkage, Flow 0.0036 cm/cm0.0036 in/in24hrs; ISO 294
 0.0030 - 0.0050 cm/cm0.0030 - 0.0050 in/in24hrs; ASTM D955
Linear Mold Shrinkage, Transverse 0.0040 - 0.0060 cm/cm0.0040 - 0.0060 in/in24hrs; ASTM D955
 0.0051 cm/cm0.0051 in/in24hrs; ISO 294
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 105 MPa15200 psiASTM D638
 107 MPa15500 psiISO 527
Elongation at Break 5.9 %5.9 %ASTM D638
 6.4 %6.4 %ISO 527
Tensile Modulus 7.68 GPa1110 ksi1 mm/min; ISO 527
 13.78 GPa1999 ksi50 mm/min; ASTM D638
Flexural Strength 158 MPa22900 psiASTM D790
 169 MPa24500 psiISO 178
Flexural Modulus 7.30 GPa1060 ksiISO 178
 7.58 GPa1100 ksiASTM D790
Izod Impact Notched 53.0 J39.1 ft-lbASTM D256
Izod Impact, Unnotched 3.73 J/cm6.99 ft-lb/inASTM D4812
Izod Impact, Notched (ISO) 8.00 kJ/m²3.81 ft-lb/in²80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 28.0 kJ/m²13.3 ft-lb/in²80*10*4; ISO 180/1U
 
Electrical PropertiesMetricEnglishComments
Surface Resistance 1000 - 1.00e+7 ohm1000 - 1.00e+7 ohmASTM D257
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  41.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
22.8 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
 41.4 µm/m-°C
@Temperature -40.0 - 40.0 °C
23.0 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
CTE, linear, Transverse to Flow  103 µm/m-°C
@Temperature -40.0 - 40.0 °C
57.2 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
 103 µm/m-°C
@Temperature -40.0 - 40.0 °C
57.2 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 150 °C302 °FFlatw 80*10*4 sp=64mm; ISO 75/Bf
 146 °C
@Thickness 3.20 mm
295 °F
@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 146 °C295 °FFlatw 80*10*4 sp=64mm; ISO 75/Af
 143 °C
@Thickness 3.20 mm
289 °F
@Thickness 0.126 in
unannealed; ASTM D648
 
Processing PropertiesMetricEnglishComments
Zone 2 310 - 320 °C590 - 608 °F
Zone 3 320 - 330 °C608 - 626 °F
Melt Temperature 305 - 325 °C581 - 617 °FInjection Molding
Mold Temperature 80.0 - 110 °C176 - 230 °F
Drying Temperature 120 °C248 °FInjection Molding
Dry Time 4.00 hour4.00 hourInjection Molding
Back Pressure 0.200 - 0.300 MPa29.0 - 43.5 psi
Screw Speed 30 - 60 rpm30 - 60 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH81256 / 289203

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.