MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
SABIC LNP™ ELCRES™ CRX9421 Polycarbonate + PBT (PC+PBT)
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced

Material Notes: LNP ELCRES CRX9421 is a semi-crystalline Polycarbonate (PC) copolymer/Polybutylene Terephthalate (PBT) opaque blend. This grade offers medium flow, UL V0 rating @ 1.5 mm, and high ductility in combination with excellent chemical resistance. It is available for custom coloring and may be an excellent candidate for a wide variety of applications that need improved chemical resistance.

Features: Enhanced Ductility,Enhanced Chemical Resistance,Flame Retardant,Colorable

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.30 g/ccASTM D792
Moisture Absorption 0.0200 %Injection Molding
Viscosity 10 cP
@Load 5.00 kg,
Temperature 250 °C
MVR cc/10 min; ASTM D1238
Linear Mold Shrinkage, Flow 0.010 - 0.016 cm/cmSABIC method
Linear Mold Shrinkage, Transverse 0.0090 - 0.016 cm/cmSABIC method
Melt Flow 11.5 g/10 min
@Load 5.00 kg,
Temperature 250 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 36.0 MPa50 mm/min; ASTM D638
Tensile Strength, Yield 44.0 MPa50 mm/min; ASTM D638
Elongation at Break 59 %50 mm/min; ASTM D638
Elongation at Yield 4.0 %50 mm/min; ASTM D638
Tensile Modulus 1985 MPa50 mm/min; ASTM D638
Flexural Strength 72.0 MPa1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 1985 MPa1.3 mm/min, 50 mm span; ASTM D790
Izod Impact Notched 590 JASTM D256
 150 J
@Temperature -30.0 °C
ASTM D256
 230 J
@Temperature 0.000 °C
ASTM D256
Izod Impact, Unnotched NBASTM D4812
 NB
@Temperature -30.0 °C
ASTM D4812
Dart Drop, Total Energy 41.0 Jpeak; ASTM D3763
 54.0 JASTM D3763
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 85.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
CTE, linear, Transverse to Flow 105 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
Deflection Temperature at 0.46 MPa (66 psi) 118 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 66.0 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Vicat Softening Point 131 °CRate B/50; ASTM D1525
 132 °CRate B/120; ASTM D1525
Flammability, UL94 V-0
@Thickness 1.50 mm
UL 94
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 240 - 255 °C
Zone 2 230 - 245 °C
Zone 3 235 - 250 °C
Melt Temperature 240 - 255 °CInjection Molding
Mold Temperature 50.0 - 70.0 °C
Drying Temperature 120 °CInjection Molding
Dry Time 2.00 - 4.00 hourInjection Molding
Back Pressure 0.300 - 0.700 MPa
Shot Size 40 - 80 %
Vent Depth 0.00250 - 0.00380 cm
Screw Speed 50 - 100 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH80589 / 288536

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.