LNP ELCRES CRX9421 is a semi-crystalline Polycarbonate (PC) copolymer/Polybutylene Terephthalate (PBT) opaque blend. This grade offers medium flow, UL V0 rating @ 1.5 mm, and high ductility in combination with excellent chemical resistance. It is available for custom coloring and may be an excellent candidate for a wide variety of applications that need improved chemical resistance. Features: Enhanced Ductility,Enhanced Chemical Resistance,Flame Retardant,Colorable Information provided by SABIC |