MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
BEWiSynbra Synterra® IM Injection molding compound
Categories: Polymer; Thermoplastic; Polylactic Acid (PLA) Biopolymer

Material Notes: Typical properties : Short cycle times (fast crystallization) - Good Impact – High temperature resistance – Good surface finish

Information provided by BEWi Synbra

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.27 g/ccPolymer; ISO 1183
Melt Flow 4.0 - 8.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 45.0 - 50.0 MPaISO 527
Elongation at Break 2.0 - 3.0 %ISO 527
Modulus of Elasticity 3.90 - 4.20 GPaISO 527
Charpy Impact Unnotched >= 89.0 kJ/m²ISO 179/1eU
Charpy Impact, Notched 4.60 kJ/m²ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 100 °Cflat; ISO 075
 123 °C0,9 MPa edge; ISO 075
Vicat Softening Point 100 °C
@Load 5.10 kg
50°C/h; ISO 306/B
 160 °C
@Load 1.02 kg
50°C/h; ISO 306/A
 
Processing PropertiesOriginal ValueComments
Processing Temperature 180 °Ccompression
 200 °Cmetering
Feed Temperature 150 °C
Nozzle Temperature 190 °C
Mold Temperature 100 - 110 °Cobligatory for high temperature performance
Drying Temperature 90.0 - 110 °C
@Time 14400 - 21600 sec
Dew Point -40.0 °F
Back Pressure 1.00 - 1.50 MPa
 
Descriptive Properties
Appearanceround pellets
ColorOff white
Screw speed0,2 – 0,4 m/sec

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PBEWS018 / 250827

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.