MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BEWiSynbra Synterra® IM Injection molding compound
Categories: Polymer; Thermoplastic; Polylactic Acid (PLA) Biopolymer

Material Notes: Typical properties : Short cycle times (fast crystallization) - Good Impact – High temperature resistance – Good surface finish

Information provided by BEWi Synbra

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.27 g/cc0.0459 lb/in³Polymer; ISO 1183
Melt Flow 4.0 - 8.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
4.0 - 8.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 45.0 - 50.0 MPa6530 - 7250 psiISO 527
Elongation at Break 2.0 - 3.0 %2.0 - 3.0 %ISO 527
Modulus of Elasticity 3.90 - 4.20 GPa566 - 609 ksiISO 527
Charpy Impact Unnotched >= 8.90 J/cm²>= 42.4 ft-lb/in²ISO 179/1eU
Charpy Impact, Notched 0.460 J/cm²2.19 ft-lb/in²ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 100 °C212 °Fflat; ISO 075
 123 °C253 °F0,9 MPa edge; ISO 075
Vicat Softening Point  100 °C
@Load 5.10 kg
212 °F
@Load 11.2 lb
50°C/h; ISO 306/B
 160 °C
@Load 1.02 kg
320 °F
@Load 2.25 lb
50°C/h; ISO 306/A
 
Processing PropertiesMetricEnglishComments
Processing Temperature 180 °C356 °Fcompression
 200 °C392 °Fmetering
Feed Temperature 150 °C302 °F
Nozzle Temperature 190 °C374 °F
Mold Temperature 100 - 110 °C212 - 230 °Fobligatory for high temperature performance
Drying Temperature 90.0 - 110 °C
@Time 14400 - 21600 sec
194 - 230 °F
@Time 4.00 - 6.00 hour
Dew Point -40.0 °C-40.0 °F
Back Pressure 1.00 - 1.50 MPa145 - 218 psi
 
Descriptive Properties
Appearanceround pellets
ColorOff white
Screw speed0,2 – 0,4 m/sec

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBEWS018 / 250827

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.