MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Duratherm XLT-120 Heat Transfer Fluid
Categories: Fluid

Material Notes: Duratherm XLT-120 heat transfer fluid does not require monitoring of concentration or additive levels. Duratherm XLT-120 utilizes an exclusive additive system for long-term, trouble-free operation at any temperature, high or low. Duratherm XLT-120 is plant and user friendly. Low odors, high flash point and no SARA reportable substances makes Duratherm XLT-120 the wise choice for worker health and safety. After its extensive service life, Duratherm XLT-120 can typically be disposed of through local waste oil recycling programs.

Information provided by Duratherm.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 50.1 lb/ft³
@Temperature 65.0 °C
ASTM D1298
 50.1 lb/ft³
@Temperature 65.0 °C
 51.2 lb/ft³
@Temperature 0.000 °C
ASTM D1298
 51.5 lb/ft³
@Temperature -15.0 °C
 51.9 lb/ft³
@Temperature -40.0 °C
ASTM D1298
 52.6 lb/ft³
@Temperature -84.0 °C
ASTM D1298
 52.7 lb/ft³
@Temperature -85.0 °C
Viscosity 0.62 cP
@Temperature 65.0 °C
Dynamic
 1.92 cP
@Temperature -15.0 °C
Dynamic
 38.86 cP
@Temperature -85.0 °C
Dynamic
Kinematic Viscosity 0.76 cSt
@Temperature 65.0 °C
ASTM D445
 1.73 cSt
@Temperature 0.000 °C
x
 2.33 cSt
@Temperature -15.0 °C
 2.48 cSt
@Temperature -18.0 °C
ASTM D445
 4.53 cSt
@Temperature -40.0 °C
ASTM D445
 44.04 cSt
@Temperature -84.0 °C
ASTM D445
 46.07 cSt
@Temperature -85.0 °C
Vapor Pressure 0.000 atm
@Temperature -120 °C
ASTM D2879
 0.000 atm
@Temperature 15.0 °C
ASTM D2879
 0.000 atm
@Temperature -85.0 °C
 0.000 atm
@Temperature -15.0 °C
 0.00170 atm
@Temperature 38.0 °C
ASTM D2879
 0.270 atm
@Temperature 65.0 °C
ASTM D2879
 
Thermal PropertiesOriginal ValueComments
Specific Heat Capacity 1.806 J/g-°C
@Temperature -84.0 °C
 1.808 J/g-°C
@Temperature -85.0 °C
 1.898 J/g-°C
@Temperature -40.0 °C
 1.954 J/g-°C
@Temperature -15.0 °C
 1.989 J/g-°C
@Temperature 0.000 °C
 2.158 J/g-°C
@Temperature 65.0 °C
 2.158 J/g-°C
@Temperature 65.0 °C
Thermal Conductivity 0.133 W/m-K
@Temperature 65.0 °C
 0.133 W/m-K
@Temperature 65.0 °C
 0.138 W/m-K
@Temperature 0.000 °C
 0.139 W/m-K
@Temperature -15.0 °C
 0.141 W/m-K
@Temperature -40.0 °C
 0.145 W/m-K
@Temperature -84.0 °C
 0.145 W/m-K
@Temperature -85.0 °C
Distillation Temperature 83.0 - 285 °C10% to 90% range; ASTM D2887
Maximum Service Temperature, Air 65.0 °CBulk/Use Temp.
 82.0 °CFilm Temp.
Minimum Service Temperature, Air -84.0 °C
Pour Point -90.0 °CASTM D97
Flash Point 49.0 °CASTM D92
Ignition Temperature 237 °CASTM E-659-78
 
Descriptive Properties
AppearanceClear liquid, slight yellow tint
Fire Point (°C)60ASTM D92

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WDURA685 / 287878

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.