Physical Properties | Metric | English | Comments |
---|
Density | 0.803 g/cc @Temperature 65.0 °C | 0.0290 lb/in³ @Temperature 149 °F |
| 0.803 g/cc @Temperature 65.0 °C | 0.0290 lb/in³ @Temperature 149 °F |
| 0.820 g/cc @Temperature 0.000 °C | 0.0296 lb/in³ @Temperature 32.0 °F |
| 0.825 g/cc @Temperature -15.0 °C | 0.0298 lb/in³ @Temperature 5.00 °F |
| 0.831 g/cc @Temperature -40.0 °C | 0.0300 lb/in³ @Temperature -40.0 °F |
| 0.843 g/cc @Temperature -84.0 °C | 0.0304 lb/in³ @Temperature -119 °F |
| 0.844 g/cc @Temperature -85.0 °C | 0.0305 lb/in³ @Temperature -121 °F |
Viscosity | 0.62 cP @Temperature 65.0 °C | 0.62 cP @Temperature 149 °F |
| 1.92 cP @Temperature -15.0 °C | 1.92 cP @Temperature 5.00 °F |
| 38.86 cP @Temperature -85.0 °C | 38.86 cP @Temperature -121 °F |
Kinematic Viscosity | 0.76 cSt @Temperature 65.0 °C | 0.76 cSt @Temperature 149 °F |
| 1.73 cSt @Temperature 0.000 °C | 1.73 cSt @Temperature 32.0 °F |
| 2.33 cSt @Temperature -15.0 °C | 2.33 cSt @Temperature 5.00 °F |
| 2.48 cSt @Temperature -18.0 °C | 2.48 cSt @Temperature -0.400 °F |
| 4.53 cSt @Temperature -40.0 °C | 4.53 cSt @Temperature -40.0 °F |
| 44.04 cSt @Temperature -84.0 °C | 44.04 cSt @Temperature -119 °F |
| 46.07 cSt @Temperature -85.0 °C | 46.07 cSt @Temperature -121 °F |
Vapor Pressure | 0.000 bar @Temperature -120 °C | 0.000 torr @Temperature -184 °F |
| 0.000 bar @Temperature 15.0 °C | 0.000 torr @Temperature 59.0 °F |
| 0.000 bar @Temperature -85.0 °C | 0.000 torr @Temperature -121 °F |
| 0.000 bar @Temperature -15.0 °C | 0.000 torr @Temperature 5.00 °F |
| 0.00172 bar @Temperature 38.0 °C | 1.29 torr @Temperature 100 °F |
| 0.274 bar @Temperature 65.0 °C | 205 torr @Temperature 149 °F |
|
Thermal Properties | Metric | English | Comments |
---|
Specific Heat Capacity | 1.806 J/g-°C @Temperature -84.0 °C | 0.4316 BTU/lb-°F @Temperature -119 °F |
| 1.808 J/g-°C @Temperature -85.0 °C | 0.4321 BTU/lb-°F @Temperature -121 °F |
| 1.898 J/g-°C @Temperature -40.0 °C | 0.4536 BTU/lb-°F @Temperature -40.0 °F |
| 1.954 J/g-°C @Temperature -15.0 °C | 0.4670 BTU/lb-°F @Temperature 5.00 °F |
| 1.989 J/g-°C @Temperature 0.000 °C | 0.4754 BTU/lb-°F @Temperature 32.0 °F |
| 2.158 J/g-°C @Temperature 65.0 °C | 0.5158 BTU/lb-°F @Temperature 149 °F |
| 2.158 J/g-°C @Temperature 65.0 °C | 0.5158 BTU/lb-°F @Temperature 149 °F |
Thermal Conductivity | 0.133 W/m-K @Temperature 65.0 °C | 0.923 BTU-in/hr-ft²-°F @Temperature 149 °F |
| 0.133 W/m-K @Temperature 65.0 °C | 0.923 BTU-in/hr-ft²-°F @Temperature 149 °F |
| 0.138 W/m-K @Temperature 0.000 °C | 0.958 BTU-in/hr-ft²-°F @Temperature 32.0 °F |
| 0.139 W/m-K @Temperature -15.0 °C | 0.965 BTU-in/hr-ft²-°F @Temperature 5.00 °F |
| 0.141 W/m-K @Temperature -40.0 °C | 0.979 BTU-in/hr-ft²-°F @Temperature -40.0 °F |
| 0.145 W/m-K @Temperature -84.0 °C | 1.01 BTU-in/hr-ft²-°F @Temperature -119 °F |
| 0.145 W/m-K @Temperature -85.0 °C | 1.01 BTU-in/hr-ft²-°F @Temperature -121 °F |
Distillation Temperature | 83.0 - 285 °C | 181 - 545 °F |
Maximum Service Temperature, Air | 65.0 °C | 149 °F |
| 82.0 °C | 180 °F |
Minimum Service Temperature, Air | -84.0 °C | -119 °F |
Pour Point | -90.0 °C | -130 °F |
Flash Point | 49.0 °C | 120 °F |
Ignition Temperature | 237 °C | 459 °F |
|
Descriptive Properties |
---|
Appearance | Clear liquid, slight yellow tint |
Fire Point (°C) | 60 |
Some of the values displayed above may have been converted from their original units and/or rounded in order to
display the information in a consistent format. Users requiring more precise data for scientific or engineering
calculations can click on the property value to see the original value as well as raw conversions to equivalent units.
We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding
error. We also ask that you refer to MatWeb's
terms of use regarding this information.
Click here to view
all the property values for this datasheet as they were originally entered into MatWeb.