MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

DuPont Teijin Films Melinex® ST557 Polyester Film, 200 Gauge
Categories: Polymer; Film; Thermoplastic; Polyester, TP; Polyester Film

Material Notes: Melinex® ST557 is a slightly hazy polyester film with low shrinkage, good flatness, and excellent handling properties. Melinex® ST557 is pretreated with a unique primer on both surfaces for adhesion in special applications

Information provided by DuPont.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 50.8 microns2.00 mil
 
Mechanical PropertiesMetricEnglishComments
Flex Crack Resistance >= 20000>= 20000Cycles; ASTM D2176
Coefficient of Friction, Static <= 0.50<= 0.50ASTM D1894
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmASTM D257
Surface Resistivity per Square 1.00e+13 ohm1.00e+13 ohmASTM D257
Dielectric Constant 2.9
@Frequency 100 Hz
2.9
@Frequency 100 Hz
ASTM D150
Dielectric Strength 197 kV/mm5000 kV/inASTM D149
Dielectric Breakdown 10000 V10000 VASTM D149
 
Thermal PropertiesMetricEnglishComments
CTE, linear 18.0 µm/m-°C
@Temperature 20.0 - 50.0 °C
10.0 µin/in-°F
@Temperature 68.0 - 122 °F
Melting Point 265 °C509 °F
Shrinkage, MD 0.15 %
@Temperature 150 °C,
Time 1800 sec
0.15 %
@Temperature 302 °F,
Time 0.500 hour
Unrestrained
Shrinkage, TD 0.15 %
@Temperature 150 °C,
Time 1800 sec
0.15 %
@Temperature 302 °F,
Time 0.500 hour
Unrestrained
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 85.5 %85.5 %TLT; ASTM D1003
 
Descriptive Properties
Coefficient of Hygroscopic Expansion0.000008 IN/IN/% RH40% - 80% RH

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
DuPont Teijin Films Melinex® SWC Polyester Film, 48 Gauge
DuPont Teijin Films Melinex® ST730 Polyester Film
DuPont Teijin Films Melinex® ST580 Polyester Film, 200 Gauge
DuPont Teijin Films Melinex® ST329 Polyester Film, 1000 Gauge
DuPont Teijin Films Melinex® ST328 Polyester Film, 1400 Gauge

PDTZ9248 / 139572

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.