MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

DuPont Teijin Films Melinex® ST730 Polyester Film
Categories: Polymer; Film; Thermoplastic; Polyester, TP; Polyester Film

Material Notes: Melinex® ST730 is an optically clear, high gloss, heat stabilized polyester film which is differentially treated on both sides. One side provides exceptional adhesion to both solvent based and UV curing inks and lacquers. The other side provides in addition to exceptional adhesion properties, unique UV Multipass exposure resilience. These characteristics make Melinex® ST730 film particularly suited for the graphics layer of membrane touch switches with a multifold exposure to UV.

Approvals: UL 94 VTM-2 - for 500, 700, 1000 gauge (0.13, 0.18, 0.25mm)

Information provided by DuPont.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.39 g/cc0.0502 lb/in³
Thickness 125 - 250 microns4.92 - 9.84 mil
 
Mechanical PropertiesMetricEnglishComments
Flexural Strength 137.9 MPa20000 psi
Coefficient of Friction 0.600.60
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+8 - 1.00e+12 ohm-cm1.00e+8 - 1.00e+12 ohm-cm
Surface Resistivity per Square 1.00e+8 ohm1.00e+8 ohm
Dielectric Constant 2.92.9
Dielectric Strength 118 kV/mm3000 kV/in
 
Thermal PropertiesMetricEnglishComments
CTE, linear 34.2 µm/m-°C
@Temperature 20.0 - 50.0 °C
19.0 µin/in-°F
@Temperature 68.0 - 122 °F
Melting Point 265 °C509 °F
Shrinkage, MD 1.0 %
@Temperature 150 °C,
Time 1800 sec
1.0 %
@Temperature 302 °F,
Time 0.500 hour
Unrestrained
Shrinkage, TD 1.0 %
@Temperature 150 °C,
Time 1800 sec
1.0 %
@Temperature 302 °F,
Time 0.500 hour
Unrestrained
 
Optical PropertiesMetricEnglishComments
Haze  1.0 %
@Thickness 0.127 mm
1.0 %
@Thickness 0.00500 in
ASTM D1003
 1.0 %
@Thickness 0.178 mm
1.0 %
@Thickness 0.00700 in
ASTM D1003
 1.2 %
@Thickness 0.254 mm
1.2 %
@Thickness 0.0100 in
ASTM D1003
Gloss 140 %140 %
Transmission, Visible 88 %88 %
 
Descriptive Properties
Coefficient of Hygroscopic Expansion0.000006 IN/IN/% RH40% - 80% RH

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
DuPont Teijin Films Melinex® ST580 Polyester Film, 200 Gauge
DuPont Teijin Films Melinex® SWC Polyester Film, 48 Gauge
DuPont Teijin Films Melinex® ST505 Polyester Film, 500 Gauge
DuPont Teijin Films Melinex® ST579 Polyester Film, 200 Gauge
DuPont Teijin Films Melinex® ST504 Polyester Film, 500 Gauge

PDTZ9251 / 139575

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.