MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

SABIC NORYL™ Resin SE1GFN3 Polyphenylene Ether + PS (PPE+PS) (Europe)
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene + Polyphenylene Ether, Unreinforced

Material Notes: NORYL™ SE1GFN3 resin is a 30% glass reinforced blend of polyphenylene ether (PPE) + high impact polystyrene (HIPS). This injection moldable grade contains non-brominated, non-chlorinated flame retardant and carries a UL94 flame rating of V1 at 1.5mm along with UL746C Outdoor Suitability rating of F1 and RTI of 110C. NORYL SE1GFN3 exhibits high heat resistance, good dielectric strength, dimensional stability, hydrolytic stability, and very low moisture absorption. This material is an excellent candidate for a variety of applications such as solar frames, unattended power supply (UPS) inverter/charger, indoor and outdoor electrical enclosures / housings / connectors, and wall plates / sockets / switches.

Features: Hydrolytic Stability,Low Creep Sensitivity,Good Stiffness,Non-Halogenated,Non-Chlorinated,Non-Brominated,Low Warpage,Structural

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.29 g/cc0.0466 lb/in³ISO 1183
Moisture Absorption 0.0700 %0.0700 %23°C / 50% RH; ISO 62
Water Absorption at Saturation 0.23 %0.23 %ISO 62-1
Viscosity 9.0 cP
@Load 10.0 kg,
Temperature 280 °C
9.0 cP
@Load 22.0 lb,
Temperature 536 °F
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.0010 - 0.0030 cm/cm0.0010 - 0.0030 in/inSABIC method
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 130 MPa18900 psiH358/30; ISO 2039-1
Tensile Strength at Break 105 MPa15200 psi5 mm/min; ISO 527
Elongation at Break 2.0 %2.0 %5 mm/min; ISO 527
Tensile Modulus 8.00 GPa1160 ksi1 mm/min; ISO 527
Flexural Strength 130 MPa18900 psibreak, 2mm/min; ISO 178
Flexural Modulus 6.00 GPa870 ksi2 mm/min; ISO 178
Izod Impact, Unnotched (ISO) 25.0 kJ/m²11.9 ft-lb/in²80*10*4; ISO 180/1U
 25.0 kJ/m²
@Temperature -30.0 °C
11.9 ft-lb/in²
@Temperature -22.0 °F
80*10*4; ISO 180/1U
Charpy Impact Unnotched 3.00 J/cm²14.3 ft-lb/in²Edgew 80*10*4 sp=62mm; ISO 179/1eU
 3.00 J/cm²
@Temperature -30.0 °C
14.3 ft-lb/in²
@Temperature -22.0 °F
Edgew 80*10*4 sp=62mm; ISO 179/1eU
Taber Abrasion, mg/1000 Cycles 5555CS-17, 1 kg; SABIC method
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmIEC 60093
Surface Resistance >= 1.00e+15 ohm>= 1.00e+15 ohmROA; IEC 60093
Dielectric Constant  3.0
@Frequency 1e+6 Hz
3.0
@Frequency 1e+6 Hz
IEC 60250
 3.1
@Frequency 50.0 - 60.0 Hz
3.1
@Frequency 50.0 - 60.0 Hz
IEC 60250
Dielectric Strength  16.0 kV/mm
@Thickness 3.20 mm
406 kV/in
@Thickness 0.126 in
in oil; IEC 60243-1
 25.0 kV/mm
@Thickness 1.60 mm
635 kV/in
@Thickness 0.0630 in
in oil; IEC 60243-1
 30.0 kV/mm
@Thickness 0.800 mm
762 kV/in
@Thickness 0.0315 in
in oil; IEC 60243-1
Dissipation Factor  0.0050
@Frequency 1e+6 Hz
0.0050
@Frequency 1e+6 Hz
IEC 60250
 0.0080
@Frequency 50.0 - 60.0 Hz
0.0080
@Frequency 50.0 - 60.0 Hz
IEC 60250
Comparative Tracking Index 175 - 250 V175 - 250 VUL 746A
 300 V300 VIEC 60112
Hot Wire Ignition, HWI >= 120 sec
@Thickness >=1.50 mm
>= 120 sec
@Thickness >=0.0591 in
UL 746A
High Amp Arc Ignition, HAI  0.00 - 15 arcs
@Thickness >=1.50 mm
0.00 - 15 arcs
@Thickness >=0.0591 in
UL 746A
 15 - 30 arcs
@Thickness >=6.00 mm
15 - 30 arcs
@Thickness >=0.236 in
UL 746A
High Voltage Arc-Tracking Rate, HVTR >= 150 mm/min>= 5.91 in/minUL 746A
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  30.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
16.7 µin/in-°F
@Temperature 73.4 - 176 °F
ISO 11359-2
 37.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
20.6 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
 37.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
20.6 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
CTE, linear, Transverse to Flow  55.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
30.6 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
 55.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
30.6 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
 70.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
38.9 µin/in-°F
@Temperature 73.4 - 176 °F
ISO 11359-2
Thermal Conductivity 0.280 W/m-K1.94 BTU-in/hr-ft²-°FISO 8302
Hot Ball Pressure Test 125 °C257 °FPASS; IEC 60695-10-2
 140 °C284 °FIEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi) 140 °C284 °FEdgew 120*10*4 sp=100mm; ISO 75/Be
Deflection Temperature at 1.8 MPa (264 psi) 135 °C275 °FEdgew 120*10*4 sp=100mm; ISO 75/Ae
Vicat Softening Point 145 °C293 °FRate B/50; ISO 306
 150 °C302 °FRate B/120; ISO 306
 155 °C311 °FRate A/50; ISO 306
UL RTI, Electrical 110 °C230 °FUL 746B
UL RTI, Mechanical with Impact 105 °C221 °FUL 746B
UL RTI, Mechanical without Impact 110 °C230 °FUL 746B
Flammability, UL94  V-1
@Thickness >=1.50 mm
V-1
@Thickness >=0.0591 in
UL 94
 V-0
@Thickness >=6.00 mm
V-0
@Thickness >=0.236 in
UL 94
 5VA
@Thickness >=3.00 mm
5VA
@Thickness >=0.118 in
UL 94
Oxygen Index 31 %31 %ISO 4589
Glow Wire Flammability Index 960 °C
@Thickness 3.20 mm
1760 °F
@Thickness 0.126 in
IEC 60695-2-12
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 280 - 300 °C536 - 572 °F
Zone 2 280 - 300 °C536 - 572 °F
Zone 3 300 - 320 °C572 - 608 °F
Melt Temperature 300 - 320 °C572 - 608 °FInjection Molding
Mold Temperature 100 - 130 °C212 - 266 °F
Drying Temperature 110 - 120 °C230 - 248 °FInjection Molding
Dry Time 2.00 - 3.00 hour2.00 - 3.00 hourInjection Molding
Precipitation Temperature 80.0 - 100 °C176 - 212 °FHopper Temperature
 
Descriptive Properties
UV-light, water exposure/immersionF2UL 746C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH82473 / 290420

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.