MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Hexcel® HexBond™ ST1040 Epoxy Paste Adhesive
Categories: Polymer; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Description: Toughened two-part adhesive, specifically designed for metal skins, composites, thermoplastic and thermosetting materials and elastomers bonding. This paste adhesive has very good performance on grinding surfaces.

Features:

  • Cure 2h at 65oC/149oF or 15 days at room temperature
  • Service temperature to 120oC/248oF
  • High shear and peel strength (even with a grinding surface
  • Good tolerance to the surfaced preparation and the type of substrate

Information provided by Hexcel Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Brookfield Viscosity 10.0 - 30.0 cPPart B
 30000 - 60000 cPPart A
 50000 cPMixed
 
Mechanical PropertiesOriginal ValueComments
Adhesive Bond Strength 4.00 MPa
@Temperature 120 °C
Lap Shear, 15 days at 23°C; EN 2243-1
 5.00 MPa
@Temperature 120 °C
Lap Shear, 2 Hours at 65°C; EN 2243-1
 18.0 MPa
@Temperature 80.0 °C
Lap Shear, 15 days at 23°C; EN 2243-1
 28.0 MPa
@Temperature 80.0 °C
Lap Shear, 2 Hours at 65°C; EN 2243-1
 37.0 MPa
@Temperature 22.8 °C
Lap Shear, 15 days at 23°C; EN 2243-1
 45.0 MPa
@Temperature 22.8 °C
Lap Shear, 2 Hours at 65°C; EN 2243-1
Peel Strength 9.60 kN/mBell, 23°C
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 MonthPart A
 12.0 MonthPart B
 
Descriptive Properties
ColorPinkMixture
 PinkPart A
 YellowPart B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PHEXCB9291 / 322447

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.