MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Hexcel® HexBond™ ST1040 Epoxy Paste Adhesive
Categories: Polymer; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Description: Toughened two-part adhesive, specifically designed for metal skins, composites, thermoplastic and thermosetting materials and elastomers bonding. This paste adhesive has very good performance on grinding surfaces.

Features:

  • Cure 2h at 65oC/149oF or 15 days at room temperature
  • Service temperature to 120oC/248oF
  • High shear and peel strength (even with a grinding surface
  • Good tolerance to the surfaced preparation and the type of substrate

Information provided by Hexcel Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Brookfield Viscosity 10.0 - 30.0 cP10.0 - 30.0 cPPart B
 30000 - 60000 cP30000 - 60000 cPPart A
 50000 cP50000 cPMixed
 
Mechanical PropertiesMetricEnglishComments
Adhesive Bond Strength  4.00 MPa
@Temperature 120 °C
580 psi
@Temperature 248 °F
Lap Shear, 15 days at 23°C; EN 2243-1
 5.00 MPa
@Temperature 120 °C
725 psi
@Temperature 248 °F
Lap Shear, 2 Hours at 65°C; EN 2243-1
 18.0 MPa
@Temperature 80.0 °C
2610 psi
@Temperature 176 °F
Lap Shear, 15 days at 23°C; EN 2243-1
 28.0 MPa
@Temperature 80.0 °C
4060 psi
@Temperature 176 °F
Lap Shear, 2 Hours at 65°C; EN 2243-1
 37.0 MPa
@Temperature 22.8 °C
5370 psi
@Temperature 73.0 °F
Lap Shear, 15 days at 23°C; EN 2243-1
 45.0 MPa
@Temperature 22.8 °C
6530 psi
@Temperature 73.0 °F
Lap Shear, 2 Hours at 65°C; EN 2243-1
Peel Strength 9.60 kN/m54.8 pliBell, 23°C
 
Processing PropertiesMetricEnglishComments
Shelf Life 12.0 Month12.0 MonthPart A
 12.0 Month12.0 MonthPart B
 
Descriptive Properties
ColorPinkMixture
 PinkPart A
 YellowPart B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PHEXCB9291 / 322447

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.