MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Greene Tweed WR™ 300 PEEK, Carbon Filled
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK); Polyetheretherketone, PEEK, Carbon Fiber Filled

Material Notes: WR®300 is a carbon-fiber reinforced compression molded PEEK often selected by pump manufacturers and users for pump bushings and case or impeller wear rings. Maximum service life is achieved in clean, lubricated and/or moist environments.

WR300 allows the pump user to increase pump efficiency by running tighter wear ring clearances while decreasing potential pump damage when pumps are cavitated or experience radial bearing failures.

Information provided by Greene Tweed.

Vendors: Ensinger TECAPEEK™ shapes are manufactured exclusively with Victrex™ PEEK polymer. The Ensinger process and Victrex resins ensure reliability, consistency, dimensional stability, and high temperature mechanical performance.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.43 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 106ASTM D785
Hardness, Shore D 93ASTM D2240
Tensile Strength at Break 19400 psiASTM D638
Elongation at Break 1.8 %ASTM D1457
Tensile Modulus 1.57e+6 psiASTM D638
Flexural Strength 30700 psiASTM D790
Flexural Modulus 1.58e+6 psiASTM D790
Compressive Strength 29300 psiASTM D695
 
Thermal PropertiesOriginal ValueComments
CTE, linear 15.3 µin/in-°F
@Temperature 22.8 - 143 °C
Deflection Temperature at 1.8 MPa (264 psi) 600 °F
 
Descriptive Properties
ColorBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Ensinger Tecapeek® XP-100 Compression Molded PEEK Compound, Bearing Grade Material with 10% Graphite, 10% PTFE, and 10% Carbon Fiber
Greene Tweed WR™ FP100 Polyketone, Reinforced
DuPont Mobility and Materials Vespel® SCP-5009 Polyimide
Ensinger Tecapeek® XP-98HT Compression Molded PEEK HT, 30% Carbon Fiber
Ensinger Tecapeek® XP-98 Compression Molded PEEK Compound, 30% Carbon Fiber

PGREEN72 / 42366

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.