MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Greene Tweed CHEMRAZ® 640 Perfluoroelastomer
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer; Rubber or Thermoset Elastomer (TSE)

Material Notes: Chemraz® 640 perfluoroelastomer is specifically developed by Greene Tweed to meet the rigorous demands of aggressive plasma systems. This product’s unique formulation provides enhanced plasma resistance in oxygen and fluorine plasma processes resulting in minimal contamination, less downtime and higher wager processing yields. Chemraz 640 is recommended for both static and dynamics, wet and dry wafer processing applications such as etch, remote plasma cleans, and deposition (CVD, HDPCVD, etc.) Chemraz 640 remains stable at service temperatures up to 554°F (290°C).

Applications:

  • Endpoint windows
  • Valve seals
  • Isolator valve seals
  • Lid seals
  • Gas inlet/outlet seals
  • Slit valve seals
  • Chamber seals
  • Gasket seals
  • Dispensing seals
  • Regulator seals
  • Filler seals

Information provided by Greene Tweed.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.08 g/cc2.08 g/ccASTM D297
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 8080ASTM D2240
Tensile Strength at Break 11.96 MPa1735 psiASTM D1414
Tensile Strength, Yield 2.41 MPa350 psi@50% Elongation; ASTM D1414
 7.688 MPa1115 psi@100% Elongation; ASTM D1414
Elongation at Break 165 %165 %ASTM D1414
Compression Set 25 %
@Temperature 204 °C,
Time 252000 sec
25 %
@Temperature 400 °F,
Time 70.0 hour
At 25% deflection; ASTM D395
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 290 °C554 °F
Minimum Service Temperature, Air -20.0 °C-4.00 °F
 
Descriptive Properties
ColorBrown

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Greene Tweed CHEMRAZ® 653 Perfluoroelastomer
Greene Tweed CHEMRAZ® 592 Perfluoroelastomer
Greene Tweed CHEMRAZ® 655 Perfluoroelastomer
Greene Tweed CHEMRAZ® 585 Perfluoroelastomer
Greene Tweed CHEMRAZ® 644 Perfluoroelastomer

PGREEN28 / 42322

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.