MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Melos Mecoline S TP 1013 F Halogen-free, thermoplastic, flame retardant sheathing
Categories: Polymer; Thermoplastic

Material Notes: Halogen-free, thermoplastic, flame retardant sheathing compound for low and medium voltage cables

Compound class: Sheathing

Compound category: TP

Flame retardant: ATH

Standards: DIN EN 50363-8 TM7; DIN VDE 0276-604 HM4; DIN VDE 0281 part 14 TM7; IEC 60092-360 SHF 1; VDE 0207 part 24 HM2, HM4; VDE 0250 part 215 HM5

Typical applications: Halogen-free, low smoke, thermoplastic, highly oil and extra fuel resistant, flame retardant compound for the sheathing of low and medium voltage cables for moving applications. (e. g. Green Energy/Offshore)

Features: Flame retardant; Halogen-free; Low smoke; Flexible; Flexible at low temperatures: Low smoke; Oil resistant

Information provided by Melos

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.61 g/ccpressed plaques, 165°C / 5 min; DIN EN ISO 1183-1A
pH >= 5.0Corrosivity, Acid gas emission; IEC 60754-2
Mooney Viscosity 58
@Temperature 160 °C
ML (1+4); DIN ISO 289-1
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 89pressed plaques, 165°C / 5 min; DIN ISO 7619-1
Tensile Strength 10.8 MPaextruded tapes; IEC 60811-501
 9.71 MPa
@Temperature 150 °C,
Time 360000 sec
extruded tapes, Fluid IRM 902; IEC 60811-404
 10.1 MPa
@Temperature 136 °C,
Time 605000 sec
extruded tapes, After ageing in air oven; IEC 60811-401
 11.502 MPa
@Temperature 90.0 °C,
Time 1.21e+6 sec
extruded tapes, Fluid IRM 902; IEC 60811-404
 11.804 MPa
@Temperature 100 °C,
Time 432000 sec
extruded tapes, Fluid IRM 902; IEC 60811-404
 12.204 MPa
@Temperature 80.0 °C,
Time 5.18e+6 sec
extruded tapes, Fluid IRM 902; IEC 60811-404
 12.6 MPa
@Temperature 80.0 °C,
Time 605000 sec
extruded tapes, After ageing in air oven; IEC 60811-401
 99.82 MPa
@Temperature 23.0 °C,
Time 86400 sec
extruded tapes, Diesel; IEC 60811-404
 101.01 MPa
@Temperature 100 °C,
Time 86400 sec
extruded tapes, Diesel; IEC 60811-404
Elongation at Break 300 %extruded tapes; IEC 60811-501
 235.8 %
@Temperature 100 °C,
Time 86400 sec
extruded tapes, Diesel; IEC 60811-404
 257.4 %
@Temperature 23.0 °C,
Time 86400 sec
extruded tapes, Diesel; IEC 60811-404
 267 %
@Temperature 136 °C,
Time 605000 sec
extruded tapes, After ageing in air oven; IEC 60811-401
 273 %
@Temperature 80.0 °C,
Time 605000 sec
extruded tapes, After ageing in air oven; IEC 60811-401
 285.9 %
@Temperature 100 °C,
Time 432000 sec
extruded tapes, Fluid IRM 902; IEC 60811-404
 291 %
@Temperature 90.0 °C,
Time 1.21e+6 sec
extruded tapes, Fluid IRM 902; IEC 60811-404
 312.9 %
@Temperature 80.0 °C,
Time 5.18e+6 sec
extruded tapes, Fluid IRM 902; IEC 60811-404
 411.3 %
@Temperature 150 °C,
Time 360000 sec
extruded tapes, Fluid IRM 902; IEC 60811-404
Penetration 12
@Temperature 90.0 °C,
Time 21600 sec
[%] Hot pressure test, extruded tapes; IEC 60811-508
 18
@Temperature 100 °C,
Time 21600 sec
[%] Hot pressure test, extruded tapes; IEC 60811-508
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 3.80e+10 ohm-cm
@Temperature 90.0 °C
500V; VDE 0303-30
 2.20e+11 ohm-cm
@Temperature 23.0 °C
500V; VDE 0303-30
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 90.0 °C
Minimum Service Temperature, Air -50.0 °C
Brittleness Temperature -42.0 °CASTM D 746
 
Processing PropertiesOriginal ValueComments
Processing Temperature 70.0 - 180 °CMaximum mass temperature
 160 - 180 °CTool
Zone 1 130 - 150 °C
Zone 2 140 - 160 °C
Zone 3 140 - 160 °C
Zone 4 150 - 170 °C
Zone 5 150 - 170 °C
Adapter Temperature 155 - 175 °C
Head Temperature 160 - 180 °C
Drying Temperature 60.0 - 70.0 °C
Dry Time 4.00 - 6.00 hour
Shelf Life 12.0 Month
 
Component Elements PropertiesOriginal ValueComments
Loss on Ignition(%) 38 %pressed plaques, 165°C / 5 min.; ASTM D 2863 A
 
Descriptive Properties
Cold bend testNo cracksat -40°C, IEC 60811-504
Conductivity<0.4 µS/mmpressed plaques, 165°C / 5 min, IEC 60754-2
Main burning properties<5 mg/gAmount of halogen acid gas, IEC 60754-1
Pulley flexing test>30000 cyclesEN 50 396 cl. 6.2
Toxicity index<1.2NES 713
 3.6ITC, EN 50305

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMELOS006 / 296113

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.