MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Fibre Glast 90 CC Isophthalic Polyester Resin (Clear Casting Properties)  (discontinued **)
Categories: Polymer; Thermoset; Polyester, TS; Polyester (Thermoset) - Rigid

Material Notes: Description:

#90 Isophthalic Polyester Resin is perfect for making dimensionally stable polyester molds, corrosive service part fabrication, and as a durable repair material for tank linings. #90 permits fast wet-out in spray or hand laminates. Its 225°F service temperature also resists exotherm and post cure problems. Properly fabricated parts may be used in food service applications. #90 is a pre-promoted, thixotropic, corrosion and temperature-resistant Isophthalic polyester resin. This versatile product features a high molecular weight and crosslink density and offers good corrosion resistance in a variety of aqueous and acidic media. The performance of #90 has been proven by over 30 years of successful service.

Features:
  • High molecular weight Isophthalic polymer
  • Contains no esterification catalyst
  • Chemical components listed under FDA 177.2420 Title 21
  • Laminates based on #90 can meet BS 6920 requirements
  • Laminates can meet MIL-R-7575C Grade A and B with Class 0 and 3 Electrical Properties
  • Manufactured using statistical controls in ISO-9002 certified plants

Benefits:
  • Corrosion resistance, Strength, Toughness
  • Superior corrosion and blister resistance
  • Can be used in food and beverage contact application
  • Approved for use in military applications
  • Consistent batch to batch performance

Properties are listed for 1/8" Clear Casting, at Room Temperature of 77°F

Information provided by Fibre Glast Developments Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Barcol 4040ASTM D2583
Tensile Strength at Break 64.1 MPa9300 psiASTM D638
Elongation at Break 2.4 %2.4 %ASTM D638
Tensile Modulus 4.76 GPa690 ksiASTM D638
Flexural Strength 114 MPa16600 psiASTM D790
Flexural Modulus 0.359 GPa52.0 ksiASTM D790
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 107.2 °C225.0 °FDeflection Temp; Load not specified; ASTM D648
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 90 %90 %clear; thickness not quantified

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Fibre Glast 90L Isophthalic Polyester Resin (Laminate Properties)
E-Glass Fiber, Generic
Bakelite® UP 802 Unsaturated Polyester Resin, High Surface Quality, Low Shrinkage, High Arc Resistance
Overview of materials for Thermoplastic Polyurethane (TPUR), Glass Fiber Reinforced
Bakelite® UP 3415 Unsaturated Polyester Resin, Low Shrinkage, High Arc Resistance, UL Listed, High Mechanical Strength

PFIBRE30 / 38296

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.