MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Bakelite® UP 802 Unsaturated Polyester Resin, High Surface Quality, Low Shrinkage, High Arc Resistance
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset; Polyester, TS; Thermoset Polyester Glass Filled BMC

Material Notes: Polyester molding compound, inorganically filled, glass fiber reinforced, styrene free, high dimensional stability, very slight post shrinkage, good mechanical properties, increased electrical values.

Applications: Ignition distributor caps, distributor fingers, spark plug connectors.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.98 g/cc0.0715 lb/in³ISO 1183
Apparent Bulk Density 0.890 g/cc0.0322 lb/in³ISO 60
Linear Mold Shrinkage 0.0020 cm/cm0.0020 in/inCompression Molding. Post Shrinkage = 0.05%.; ISO 2577
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 360 MPa52200 psiH961/30; ISO 2039/P1
Flexural Strength 100 MPa14500 psiISO 178
Flexural Modulus 12.5 GPa1810 ksiISO 178
Compressive Strength 210 MPa30500 psiISO 604
Charpy Impact Unnotched 0.650 J/cm²3.09 ft-lb/in²ISO 179-1 eU
Charpy Impact, Notched 0.350 J/cm²1.67 ft-lb/in²ISO 179-1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+13 ohm-cm1.00e+13 ohm-cm
Surface Resistance 1.00e+12 ohm1.00e+12 ohm
Dielectric Constant 5.5
@Frequency 100 Hz
5.5
@Frequency 100 Hz
Dielectric Strength 26.0 kV/mm
@Thickness 1.00 mm
660 kV/in
@Thickness 0.0394 in
IEC 60243-P1
Dissipation Factor 0.020
@Frequency 100 Hz
0.020
@Frequency 100 Hz
Comparative Tracking Index 600 V600 V
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 170 °C338 °F<20000 hours; IEC 60216-P1
 210 °C410 °F< 50 hours; IEC 60216-P1
Deflection Temperature at 8.0 MPa 180 °C356 °FISO 75-2
 
Processing PropertiesMetricEnglishComments
Feed Temperature 60.0 - 70.0 °C140 - 158 °FInjection molding
Nozzle Temperature 70.0 - 100 °C158 - 212 °FInjection molding
Melt Temperature 70.0 - 100 °C158 - 212 °FInjection molding
Mold Temperature 160 - 180 °C320 - 356 °FInjection molding
 160 - 180 °C320 - 356 °FCompression molding
Injection Pressure >= 10.0 MPa>= 1450 psiCompression and injection cavity mold pressure
Back Pressure 0.500 - 1.00 MPa72.5 - 145 psiInjection molding
Cure Time 0.167 - 0.333 min0.00278 - 0.00556 hourPer 1 mm of wall thickness, injection molding
 0.333 - 0.667 min0.00556 - 0.0111 hourPer 1 mm of wall thickness, compression molding
 
Descriptive Properties
Creep Rupture StrengthGood
Holding PressureApproximately 40-60% of injection pressure
Media ResistanceMedium
Thermal ExpansionVery Slight
Water absorption (mg)2524h / 23°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Calcium Carbonate, Calcite (CaCO3)
Bakelite® UP 804 Unsaturated Polyester Resin, High Surface Quality, UL Listed, Low Shrinkage, High Arc Resistance
Menzolit Menzolit® BMC 0160 Unsaturated Polyester UP
Bakelite® UP 3415 Unsaturated Polyester Resin, Low Shrinkage, High Arc Resistance, UL Listed, High Mechanical Strength
MarkeTech Calcium Carbonate, Calcite (CaCO3) Optical Grade Crystal

PBAKE047 / 27081

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.