MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Flame Retardant adhesives

(Viewing data as-entered. Click here to return)
Caplinq LINQTAPE™ PIT1N-CR 1 mil high temperature corona resistant polyimide film
Categories: Polymer; Adhesive; Thermoset; Polyimide, TS; Polyimide, Thermoset Film

Material Notes: LINQTAPE™PIT1N-CR Series is a high performance, high-temperature resistant polyimide film designed specifically to with stand the damaging effect of Corona. It isused in transformers, electrical rotating machines, traction motors, generators, high-temperature or high voltage coils and other insulation application where corona is a concern. LINQTAPE™PIT1N-CR Series polyimide film not only maintains its excellent physical, electrical, thermal, mechanical, and chemical properties, but also has good corona resistance and thermal conductivity. At a voltage stress of 20KV/mm (500V/mil), LINQTAPE™ PIT1N-CR has a life endurance of many hundreds of times the standard PIT1N film. LINQTAPE™PIT1N-CR Series Film comes in 33meter (36yard) length rolls of varying widths. The base polyimide film (backing) thickness is 1mil (25.4±2µm) thick. Custom thicknesses are available upon request.

Applications:

  • Traction motors
  • Transformers
  • Generators
  • Electrical rotating machines
  • Insulating magnet wire
  • Insulating circuit boards and coils
  • Insulating applications where corona is a concern

Information provided by Caplinq

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.51 g/cc
Thickness 5.00 milFilm (Backing)
 
Mechanical PropertiesOriginal ValueComments
Elongation at Break >= 40 %rupture
Film Tensile Strength at Break, MD >= 135 MPa
Film Tensile Strength at Break, TD >= 135 MPa
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cm
Surface Resistance 1.00e+15 ohm
Dielectric Constant <= 3.9
@Frequency 48.0 - 62.0 Hz
Dielectric Strength >= 5080 V/mil
Dissipation Factor <= 0.0035
@Frequency 48.0 - 62.0 Hz
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Inert 260 °C
Flammability, UL94 V-0
 
Descriptive Properties
ColorAmber
Corona resistance>80 hrat 1kV at 20kHz; 90±2°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCAPL1002 / 256002

Flame Retardant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.