MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
SABIC NORYL™ Resin N225X Polyphenylene Ether + PS (PPE+PS)
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene + Polyphenylene Ether, Unreinforced

Material Notes: NORYL™ N225X resin is a non-reinforced blend of polyphenylene ether (PPE) + high impact polystyrene (HIPS). This injection moldable grade contains non-brominated, non-chlorinated flame retardant and carries a UL94 flame rating of 5VA at 3mm and V0 at 1.5mm along with a UL746C Outdoor Suitability rating of F1. NORYL N225X resin offers good dielectric strength and strong electrical performance in addition to low moisture absorption and dimensional stability, This material is an excellent candidate for both indoor and outdoor electrical applications.

Features: Hydrolytic Stability,Low Creep Sensitivity,Flame Retardant,Non-Halogenated,Non-Brominated,Low Warpage

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.11 g/ccASTM D792
Moisture Absorption 0.0200 %Injection Molding
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm
@Thickness 3.20 mm
SABIC method
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cm
@Thickness 3.20 mm
SABIC method
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 49.0 MPa50 mm/min; ASTM D638
Tensile Strength, Yield 66.0 MPa50 mm/min; ASTM D638
Elongation at Break 17 %50 mm/min; ASTM D638
Elongation at Yield 8.0 %50 mm/min; ASTM D638
Flexural Strength 99.0 MPayld, 2.6 mm/min, 100 mm span; ASTM D790
Flexural Modulus 2490 MPa2.6 mm/min, 100 mm span; ASTM D790
Izod Impact Notched 186 JASTM D256
 96.0 J
@Temperature -30.0 °C
ASTM D256
 886 J
@Thickness 3.20 mm
reverse notched; ASTM D256
Dart Drop, Total Energy 39.0 Jpeak; ASTM D3763
 11.0 J
@Temperature -30.0 °C
peak; ASTM D3763
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 2.80e+16 ohm-cmASTM D257
Surface Resistance >= 1.00e+14 ohmASTM D257
Dielectric Constant 2.55
@Frequency 1e+6 Hz
ASTM D150
 2.69
@Frequency 50.0 - 60.0 Hz
ASTM D150
Dielectric Strength 16.2 kV/mm
@Thickness 3.20 mm
in oil; ASTM D149
Dissipation Factor 0.0070
@Frequency 1e+6 Hz
ASTM D150
 0.010
@Frequency 50.0 - 60.0 Hz
ASTM D150
Arc Resistance 60 - 120 secASTM D495
Comparative Tracking Index 400 - 600 VUL 746A
Hot Wire Ignition, HWI 60 - 120 sec
@Thickness >=1.50 mm
UL 746A
 >= 120 sec
@Thickness >=6.00 mm
UL 746A
High Amp Arc Ignition, HAI >= 120 arcs
@Thickness >=1.50 mm
UL 746A
High Voltage Arc-Tracking Rate, HVTR >= 150 mm/minUL 746A
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 109 °C
@Thickness 6.40 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 99.0 °C
@Thickness 6.40 mm
unannealed; ASTM D648
Vicat Softening Point 128 °CRate B/50; ASTM D1525
UL RTI, Electrical 95.0 °CUL 746B
UL RTI, Mechanical with Impact 80.0 °CUL 746B
UL RTI, Mechanical without Impact 95.0 °CUL 746B
Flammability, UL94 HB
@Thickness >=0.400 mm
UL 94
 V-0
@Thickness >=1.50 mm
UL 94
 5VA
@Thickness >=3.00 mm
UL 94
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 260 - 290 °C
Zone 2 240 - 280 °C
Zone 3 250 - 290 °C
Melt Temperature 260 - 290 °CInjection Molding
Mold Temperature 70.0 - 95.0 °C
Drying Temperature 95.0 - 100 °CInjection Molding
Dry Time 3.00 - 4.00 hourInjection Molding
 8.00 hourCumulative; Injection Molding
Back Pressure 0.300 - 0.700 MPa
Shot Size 30 - 70 %
Vent Depth 0.00380 - 0.00510 cm
Screw Speed 20 - 100 rpm
 
Descriptive Properties
Radiant Panel ListingTRUEUL Tested
UV-light, water exposure/immersionF1UL 746C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH82366 / 290313

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.