MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

SABIC NORYL™ Resin N225X Polyphenylene Ether + PS (PPE+PS)
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene + Polyphenylene Ether, Unreinforced

Material Notes: NORYL™ N225X resin is a non-reinforced blend of polyphenylene ether (PPE) + high impact polystyrene (HIPS). This injection moldable grade contains non-brominated, non-chlorinated flame retardant and carries a UL94 flame rating of 5VA at 3mm and V0 at 1.5mm along with a UL746C Outdoor Suitability rating of F1. NORYL N225X resin offers good dielectric strength and strong electrical performance in addition to low moisture absorption and dimensional stability, This material is an excellent candidate for both indoor and outdoor electrical applications.

Features: Hydrolytic Stability,Low Creep Sensitivity,Flame Retardant,Non-Halogenated,Non-Brominated,Low Warpage

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.11 g/cc1.11 g/ccASTM D792
Moisture Absorption 0.0200 %0.0200 %Injection Molding
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm
@Thickness 3.20 mm
0.0050 - 0.0070 in/in
@Thickness 0.126 in
SABIC method
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cm
@Thickness 3.20 mm
0.0050 - 0.0070 in/in
@Thickness 0.126 in
SABIC method
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 49.0 MPa7110 psi50 mm/min; ASTM D638
Tensile Strength, Yield 66.0 MPa9570 psi50 mm/min; ASTM D638
Elongation at Break 17 %17 %50 mm/min; ASTM D638
Elongation at Yield 8.0 %8.0 %50 mm/min; ASTM D638
Flexural Strength 99.0 MPa14400 psiyld, 2.6 mm/min, 100 mm span; ASTM D790
Flexural Modulus 2.49 GPa361 ksi2.6 mm/min, 100 mm span; ASTM D790
Izod Impact Notched 186 J137 ft-lbASTM D256
 96.0 J
@Temperature -30.0 °C
70.8 ft-lb
@Temperature -22.0 °F
ASTM D256
 886 J
@Thickness 3.20 mm
653 ft-lb
@Thickness 0.126 in
reverse notched; ASTM D256
Dart Drop, Total Energy 39.0 J28.8 ft-lbpeak; ASTM D3763
 11.0 J
@Temperature -30.0 °C
8.11 ft-lb
@Temperature -22.0 °F
peak; ASTM D3763
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 2.80e+16 ohm-cm2.80e+16 ohm-cmASTM D257
Surface Resistance >= 1.00e+14 ohm>= 1.00e+14 ohmASTM D257
Dielectric Constant  2.55
@Frequency 1e+6 Hz
2.55
@Frequency 1e+6 Hz
ASTM D150
 2.69
@Frequency 50.0 - 60.0 Hz
2.69
@Frequency 50.0 - 60.0 Hz
ASTM D150
Dielectric Strength 16.2 kV/mm
@Thickness 3.20 mm
411 kV/in
@Thickness 0.126 in
in oil; ASTM D149
Dissipation Factor  0.0070
@Frequency 1e+6 Hz
0.0070
@Frequency 1e+6 Hz
ASTM D150
 0.010
@Frequency 50.0 - 60.0 Hz
0.010
@Frequency 50.0 - 60.0 Hz
ASTM D150
Arc Resistance 60 - 120 sec60 - 120 secASTM D495
Comparative Tracking Index 400 - 600 V400 - 600 VUL 746A
Hot Wire Ignition, HWI  60 - 120 sec
@Thickness >=1.50 mm
60 - 120 sec
@Thickness >=0.0591 in
UL 746A
 >= 120 sec
@Thickness >=6.00 mm
>= 120 sec
@Thickness >=0.236 in
UL 746A
High Amp Arc Ignition, HAI >= 120 arcs
@Thickness >=1.50 mm
>= 120 arcs
@Thickness >=0.0591 in
UL 746A
High Voltage Arc-Tracking Rate, HVTR >= 150 mm/min>= 5.91 in/minUL 746A
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 109 °C
@Thickness 6.40 mm
228 °F
@Thickness 0.252 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 99.0 °C
@Thickness 6.40 mm
210 °F
@Thickness 0.252 in
unannealed; ASTM D648
Vicat Softening Point 128 °C262 °FRate B/50; ASTM D1525
UL RTI, Electrical 95.0 °C203 °FUL 746B
UL RTI, Mechanical with Impact 80.0 °C176 °FUL 746B
UL RTI, Mechanical without Impact 95.0 °C203 °FUL 746B
Flammability, UL94  HB
@Thickness >=0.400 mm
HB
@Thickness >=0.0157 in
UL 94
 V-0
@Thickness >=1.50 mm
V-0
@Thickness >=0.0591 in
UL 94
 5VA
@Thickness >=3.00 mm
5VA
@Thickness >=0.118 in
UL 94
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 260 - 290 °C500 - 554 °F
Zone 2 240 - 280 °C464 - 536 °F
Zone 3 250 - 290 °C482 - 554 °F
Melt Temperature 260 - 290 °C500 - 554 °FInjection Molding
Mold Temperature 70.0 - 95.0 °C158 - 203 °F
Drying Temperature 95.0 - 100 °C203 - 212 °FInjection Molding
Dry Time 3.00 - 4.00 hour3.00 - 4.00 hourInjection Molding
 8.00 hour8.00 hourCumulative; Injection Molding
Back Pressure 0.300 - 0.700 MPa43.5 - 102 psi
Shot Size 30 - 70 %30 - 70 %
Vent Depth 0.00380 - 0.00510 cm0.00150 - 0.00201 in
Screw Speed 20 - 100 rpm20 - 100 rpm
 
Descriptive Properties
Radiant Panel ListingTRUEUL Tested
UV-light, water exposure/immersionF1UL 746C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH82366 / 290313

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.