MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Chevron Phillips DRISCOPLEX® 6500 Series MDPE Pipe
Categories: Polymer; Thermoplastic; Polyethylene (PE); Medium Density (MDPE)

Material Notes: DriscoPlex® 6500 Series Pipe meets or exceeds:
ASTM D2513, D2683, D3261
CAN/CSA-B137.4
UPC
ASTM D3350, cell classificationPE234373E and PE234375E
PPI TR-4 designations PE2708 and PE80

DriscoPlex® 6500 Series Pipe for:
Natural Gas Distribution, LPG and Propane Gas Distribution, Yard Gas
Iron Pipe Size OD (IPS) ½" to 12"
Copper Tube Size OD (CTS) ½" to 1¼"

Information provided by Chevron Phillips Chemical Company LP.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.939 g/ccASTM D1505
Melt Flow 0.180 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
PENT >= 2000 hourASTM F1473
Tensile Strength, Yield 2800 psiASTM D638 Type IV
Elongation at Break 800 %2 in / min., Type IV Bar; ASTM D638
Flexural Modulus >= 90000 psi2% Secant; ASTM D790
Hydrostatic Design Basis 800 psi
@Temperature 60.0 °C
ASTM D2837
 1250 psi
@Temperature 23.0 °C
ASTM D2837
 
Descriptive Properties
ColorYellow
Rapid Crack Propagation123 psi0°C, ISO 13478

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCHEVC8807 / 323310

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.