MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Chevron Phillips DRISCOPLEX® 6500 Series MDPE Pipe
Categories: Polymer; Thermoplastic; Polyethylene (PE); Medium Density (MDPE)

Material Notes: DriscoPlex® 6500 Series Pipe meets or exceeds:
ASTM D2513, D2683, D3261
CAN/CSA-B137.4
UPC
ASTM D3350, cell classificationPE234373E and PE234375E
PPI TR-4 designations PE2708 and PE80

DriscoPlex® 6500 Series Pipe for:
Natural Gas Distribution, LPG and Propane Gas Distribution, Yard Gas
Iron Pipe Size OD (IPS) ½" to 12"
Copper Tube Size OD (CTS) ½" to 1¼"

Information provided by Chevron Phillips Chemical Company LP.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.939 g/cc0.0339 lb/in³ASTM D1505
Melt Flow 0.180 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.180 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
PENT >= 2000 hour>= 2000 hourASTM F1473
Tensile Strength, Yield 19.3 MPa2800 psiASTM D638 Type IV
Elongation at Break 800 %800 %2 in / min., Type IV Bar; ASTM D638
Flexural Modulus >= 0.621 GPa>= 90.0 ksi2% Secant; ASTM D790
Hydrostatic Design Basis  5.52 MPa
@Temperature 60.0 °C
800 psi
@Temperature 140 °F
ASTM D2837
 8.62 MPa
@Temperature 23.0 °C
1250 psi
@Temperature 73.4 °F
ASTM D2837
 
Descriptive Properties
ColorYellow
Rapid Crack Propagation123 psi0°C, ISO 13478

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCHEVC8807 / 323310

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.