It’s a semi-crystalline fully-fluorinated melt processable fluoropolymer which offer the highest temperature rating and broadest chemical resistance of all melt processable fluoropolymers. It is an ideal choice for extreme thermal and chemical environments. MFA exhibits the outstanding thermal behaviour and chemical resistance found in PTFE, PFA and FEP. In addition, parts made with MFA have been shown to have smooth finished surfaces. This makes MFA a good candidate for the semiconductor, electronics and biologic applications.Information provided by Guarniflon® |