MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Carpenter Custom 630 (17-Cr-4Ni) Precipitation Hardening Stainless Steel, Condition H 1100 (Heated 593°C)
Categories: Metal; Ferrous Metal; Stainless Steel; Precipitation Hardening Stainless; T S10000 Series Stainless Steel

Material Notes: Data provided by Carpenter Technology Corporation.

Custom 630 (17Cr-4Ni) is a martensitic precipitation/age-hardening stainless steel offering high strength and hardness along with excellent corrosion resistance. It has good fabricating characteristics and can be age hardened by a single-step, low temperature treatment. It has been used for a variety of applications including oil field valve parts, chemical process equipment, aircraft fittings, fasteners, pump shafts, nuclear reactor components, gears, paper mill equipment, missile fittings, and jet engine parts. Project 70® stainless Custom 630 is an improved machinability modification.

Key Words: AISI 630; UNS S17400; 17-4PH, 17/4PH, 17-4 PH, Precipitation Hardening PH Stainless Steel, 17-4
Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 7.81 g/cc0.282 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 1034 MPa150000 psi
 1331 MPa
@Temperature 0.000 °C
193000 psi
@Temperature 32.0 °F
 1440 MPa
@Temperature -40.0 °C
209000 psi
@Temperature -40.0 °F
 1441 MPa
@Temperature -62.0 °C
209000 psi
@Temperature -79.6 °F
 1710 MPa
@Temperature -196 °C
248000 psi
@Temperature -321 °F
Tensile Strength, Yield 931 MPa
@Strain 0.2 %
135000 psi
@Strain 0.2 %
 1262 MPa
@Strain 0.2 %,
Temperature 0.000 °C
183000 psi
@Strain 0.2 %,
Temperature 32.0 °F
 1303 MPa
@Strain 0.2 %,
Temperature -40.0 °C
189000 psi
@Strain 0.2 %,
Temperature -40.0 °F
 1351 MPa
@Strain 0.2 %,
Temperature -62.0 °C
195900 psi
@Strain 0.2 %,
Temperature -79.6 °F
 1675 MPa
@Strain 0.2 %,
Temperature -196 °C
242900 psi
@Strain 0.2 %,
Temperature -321 °F
Elongation at Break 17 %17 %In 50 mm
 8.0 %
@Temperature -196 °C
8.0 %
@Temperature -321 °F
In 50 mm
 15 %
@Temperature -62.0 °C
15 %
@Temperature -79.6 °F
In 50 mm
 16 %
@Temperature -40.0 °C
16 %
@Temperature -40.0 °F
In 50 mm
 16 %
@Temperature 0.000 °C
16 %
@Temperature 32.0 °F
In 50 mm
Modulus of Elasticity 197 GPa28600 ksi
Poissons Ratio 0.2720.272
Shear Modulus 77.4 GPa11200 ksiCalculated
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000770 ohm-cm0.0000770 ohm-cmfor condition H 900
 
Thermal PropertiesMetricEnglishComments
CTE, linear  11.5 µm/m-°C
@Temperature 21.0 - 93.0 °C
6.39 µin/in-°F
@Temperature 69.8 - 199 °F
 12.2 µm/m-°C
@Temperature 21.0 - 316 °C
6.78 µin/in-°F
@Temperature 69.8 - 601 °F
 12.5 µm/m-°C
@Temperature 21.0 - 427 °C
6.94 µin/in-°F
@Temperature 69.8 - 801 °F
Specific Heat Capacity 0.419 J/g-°C
@Temperature 0.000 - 100 °C
0.100 BTU/lb-°F
@Temperature 32.0 - 212 °F
condition H 900
Thermal Conductivity  17.9 W/m-K
@Temperature 149 °C
124 BTU-in/hr-ft²-°F
@Temperature 300 °F
condition H 900
 22.6 W/m-K
@Temperature 482 °C
157 BTU-in/hr-ft²-°F
@Temperature 900 °F
condition H 900
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.070 %<= 0.070 %
Chromium, Cr 15 - 17.5 %15 - 17.5 %
Copper, Cu 3.0 - 5.0 %3.0 - 5.0 %
Iron, Fe 73 %73 %as remainder
Manganese, Mn <= 1.0 %<= 1.0 %
Nb + Ta 0.15 - 0.45 %0.15 - 0.45 %
Nickel, Ni 3.0 - 5.0 %3.0 - 5.0 %
Niobium, Nb (Columbium, Cb) <= 0.45 %<= 0.45 %
Phosphorus, P <= 0.040 %<= 0.040 %
Silicon, Si <= 1.0 %<= 1.0 %
Sulfur, S <= 0.030 %<= 0.030 %
Tantalum, Ta <= 0.45 %<= 0.45 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Carpenter Custom 630 (17-Cr-4Ni) Precipitation Hardening Stainless Steel, Condition H 900 (Age-Hardened 482°C/1hr/AC)
Carpenter Custom 630 (17-Cr-4Ni) Precipitation Hardening Stainless Steel, Condition H 1150 (Heated 621°C)
Kinetics MIM 17-4PH Stainless Steel (H1100 Condition)
Carpenter Custom 630 (17-Cr-4Ni) Precipitation Hardening Stainless Steel, Condition H 1025 (Heated 552°C)
Carpenter Custom 630 (17-Cr-4Ni) Precipitation Hardening Stainless Steel, Annealed

NCARHA / 15777

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.