Physical Properties | Metric | English | Comments |
---|
Specific Gravity | 1.27 g/cc | 1.27 g/cc |
|
Mechanical Properties | Metric | English | Comments |
---|
Hardness, Shore A | 82 | 82 |
| 68 @Temperature 23.0 °C, Time 252000 sec | 68 @Temperature 73.4 °F, Time 70.0 hour |
| 71 @Temperature 23.0 °C, Time 252000 sec | 71 @Temperature 73.4 °F, Time 70.0 hour |
| 80 @Temperature 100 °C, Time 252000 sec | 80 @Temperature 212 °F, Time 70.0 hour |
| 80 @Temperature 100 °C, Time 252000 sec | 80 @Temperature 212 °F, Time 70.0 hour |
| 81 @Temperature 23.0 °C, Time 252000 sec | 81 @Temperature 73.4 °F, Time 70.0 hour |
| 81 @Temperature 125 °C, Time 252000 sec | 81 @Temperature 257 °F, Time 70.0 hour |
| 81 @Temperature 150 °C, Time 252000 sec | 81 @Temperature 302 °F, Time 70.0 hour |
| 85 @Temperature 100 °C, Time 252000 sec | 85 @Temperature 212 °F, Time 70.0 hour |
| 86 @Temperature 150 °C, Time 252000 sec | 86 @Temperature 302 °F, Time 70.0 hour |
| 87 @Temperature 125 °C, Time 252000 sec | 87 @Temperature 257 °F, Time 70.0 hour |
| 87 @Temperature 100 °C, Time 252000 sec | 87 @Temperature 212 °F, Time 70.0 hour |
| 91 @Temperature 125 °C, Time 252000 sec | 91 @Temperature 257 °F, Time 70.0 hour |
| 94 @Temperature 125 °C, Time 252000 sec | 94 @Temperature 257 °F, Time 70.0 hour |
Tensile Strength | 15.91 MPa | 2308 psi |
| 13.112 MPa @Temperature 23.0 °C, Time 252000 sec | 1901.8 psi @Temperature 73.4 °F, Time 70.0 hour |
| 13.733 MPa @Temperature 23.0 °C, Time 252000 sec | 1991.8 psi @Temperature 73.4 °F, Time 70.0 hour |
| 16.136 MPa @Temperature 23.0 °C, Time 252000 sec | 2340.3 psi @Temperature 73.4 °F, Time 70.0 hour |
| 16.693 MPa @Temperature 100 °C, Time 252000 sec | 2421.1 psi @Temperature 212 °F, Time 70.0 hour |
| 17.250 MPa @Temperature 150 °C, Time 252000 sec | 2501.9 psi @Temperature 302 °F, Time 70.0 hour |
| 17.345 MPa @Temperature 150 °C, Time 252000 sec | 2515.7 psi @Temperature 302 °F, Time 70.0 hour |
| 17.4089 MPa @Temperature 100 °C, Time 252000 sec | 2524.95 psi @Temperature 212 °F, Time 70.0 hour |
| 17.520 MPa @Temperature 125 °C, Time 252000 sec | 2541.1 psi @Temperature 257 °F, Time 70.0 hour |
| 17.5680 MPa @Temperature 100 °C, Time 252000 sec | 2548.03 psi @Temperature 212 °F, Time 70.0 hour |
| 18.1409 MPa @Temperature 125 °C, Time 252000 sec | 2631.12 psi @Temperature 257 °F, Time 70.0 hour |
| 18.363 MPa @Temperature 125 °C, Time 252000 sec | 2663.4 psi @Temperature 257 °F, Time 70.0 hour |
| 18.47511 MPa @Temperature 125 °C, Time 252000 sec | 2679.588 psi @Temperature 257 °F, Time 70.0 hour |
Elongation, Ultimate | 280 % | 280 % |
| 168 % @Temperature 125 °C, Time 252000 sec | 168 % @Temperature 257 °F, Time 70.0 hour |
| 201.1 % @Temperature 23.0 °C, Time 252000 sec | 201.1 % @Temperature 73.4 °F, Time 70.0 hour |
| 205.2 % @Temperature 150 °C, Time 252000 sec | 205.2 % @Temperature 302 °F, Time 70.0 hour |
| 206.1 % @Temperature 23.0 °C, Time 252000 sec | 206.1 % @Temperature 73.4 °F, Time 70.0 hour |
| 220.1 % @Temperature 150 °C, Time 252000 sec | 220.1 % @Temperature 302 °F, Time 70.0 hour |
| 231 % @Temperature 100 °C, Time 252000 sec | 231 % @Temperature 212 °F, Time 70.0 hour |
| 236.88 % @Temperature 125 °C, Time 252000 sec | 236.88 % @Temperature 257 °F, Time 70.0 hour |
| 241.92 % @Temperature 125 °C, Time 252000 sec | 241.92 % @Temperature 257 °F, Time 70.0 hour |
| 264.1 % @Temperature 100 °C, Time 252000 sec | 264.1 % @Temperature 212 °F, Time 70.0 hour |
| 281.12 % @Temperature 100 °C, Time 252000 sec | 281.12 % @Temperature 212 °F, Time 70.0 hour |
| 290.92 % @Temperature 23.0 °C, Time 252000 sec | 290.92 % @Temperature 73.4 °F, Time 70.0 hour |
| 407.1 % @Temperature 125 °C, Time 252000 sec | 407.1 % @Temperature 257 °F, Time 70.0 hour |
100% Modulus | 7.853 MPa | 1139 psi |
Tear Strength | 42.4 kN/m | 242 pli |
| 57.0 kN/m | 325 pli |
Compression Set | 5.4 % @Temperature 100 °C, Time 79200 sec | 5.4 % @Temperature 212 °F, Time 22.0 hour |
| 8.4 % @Temperature 100 °C, Time 252000 sec | 8.4 % @Temperature 212 °F, Time 70.0 hour |
| 12.7 % @Temperature 100 °C, Time 79200 sec | 12.7 % @Temperature 212 °F, Time 22.0 hour |
| 17.5 % @Temperature 100 °C, Time 252000 sec | 17.5 % @Temperature 212 °F, Time 70.0 hour |
|
Thermal Properties | Metric | English | Comments |
---|
Shrinkage | -8.50 % @Temperature 125 °C, Time 252000 sec | -8.50 % @Temperature 257 °F, Time 70.0 hour |
| -7.60 % @Temperature 150 °C, Time 252000 sec | -7.60 % @Temperature 302 °F, Time 70.0 hour |
| -5.70 % @Temperature 100 °C, Time 252000 sec | -5.70 % @Temperature 212 °F, Time 70.0 hour |
| -0.300 % @Temperature 23.0 °C, Time 252000 sec | -0.300 % @Temperature 73.4 °F, Time 70.0 hour |
| 0.010 % @Temperature 100 °C, Time 252000 sec | 0.010 % @Temperature 212 °F, Time 70.0 hour |
| 1.1 % @Temperature 125 °C, Time 252000 sec | 1.1 % @Temperature 257 °F, Time 70.0 hour |
| 2.4 % @Temperature 150 °C, Time 252000 sec | 2.4 % @Temperature 302 °F, Time 70.0 hour |
| 3.3 % @Temperature 100 °C, Time 252000 sec | 3.3 % @Temperature 212 °F, Time 70.0 hour |
| 18.4 % @Temperature 23.0 °C, Time 252000 sec | 18.4 % @Temperature 73.4 °F, Time 70.0 hour |
| 30.6 % @Temperature 23.0 °C, Time 252000 sec | 30.6 % @Temperature 73.4 °F, Time 70.0 hour |
|
Descriptive Properties |
---|
Color | Black |